• PD 6510:1983

    Withdrawn A Withdrawn Standard is one, which is removed from sale, and its unique number can no longer be used. The Standard can be withdrawn and not replaced, or it can be withdrawn and replaced by a Standard with a different number.

    A review of the present state of the art of assessing remanent life of pressure vessels and pressurized systems designed for high temperature service

    Available format(s):  Hardcopy, PDF

    Withdrawn date:  02-08-2013

    Language(s):  English

    Published date:  31-03-1983

    Publisher:  British Standards Institution

    Add To Cart

    Table of Contents - (Show below) - (Hide below)

    Foreword
    Committees responsible
    Section one. The background to remanent life
    assessment
       Introduction to topics covered in the other sections.
    Section two. Operating history
       Maintenance history, expired fraction of life,
       preliminary screening, rigorous analysis of critical
       areas, measurement of metal temperatures, calculation
       of stress levels, use of creep rupture data, life
       fraction rule, accuracy of estimates of fractional
       life
    Section three. Physical examination and interpretation
    of observations
       Visual inspection, non-destructive testing,
       dimensional checks, timing of examinations,
       interpretation of observations, estimation of
       remanent life from measurements, use of creep data,
       determining the cause of cracking
    Section four. Metallographic techniques
       Use of small samples or in-situ techniques,
       measurement of microstructural features controlling
       creep, measurement of cavitation or cracking,
       application of proving data, effects of condition of
       starting material
    Section five. Post-exposure tests
       Use of on-going research data, selection of suitable
       test procedure, tensile tests, fatigue tests, creep
       tests, life fraction rule, accuracy of estimates of
       remaining life
    Section six. Environmental effects
       Effects of environmental attack on the creep rate of
       materials, deviations from predicted rates of attack,
       effects of corrosion allowances, examples of
       environmental attack, transient environmental
       conditions, consequences of attack
    Section seven. Combined creep and fatigue
       Behaviour under conditions of creep or fatigue alone,
       reduction of life due to combined effects,
       simplification of analyses of effects, degree of
       interaction of creep and fatigue, available data, use
       of material examination and testing
    Section eight. Statistical methods
       Application to a large number of identical
       components, acceptance of a limited number of
       failures, scatter of parameters and resulting
       uncertainties, prediction of failure rates,
       constraints on the successful application of the
       technique
    References
    Figures
    1 Rupture life of damaged material compared with new
       material (1Cr1/2Mo); increased stress tests,
       temperature 557 deg C
    2 Rupture life of damaged material compared with new
       material (1Cr1/2Mo); increased temperature tests,
       stress 66 N/mm2
    3 Cumulative number of failed tubes versus time

    Abstract - (Show below) - (Hide below)

    Review of the techniques which are available to demonstrate the continuing fitness for purpose of high temperature pressurized systems, including the use of operating history, physical examination and interpretation of observations, metallographic techniques, post exposure tests, environment effects, creep and fatigue, and statistical methods.

    General Product Information - (Show below) - (Hide below)

    Committee PVE/1
    Development Note Inactive for the new design. (12/2009)
    Document Type Standard
    Publisher British Standards Institution
    Status Withdrawn

    Standards Referenced By This Book - (Show below) - (Hide below)

    BS 3843-3:1992 Guide to terotechnology (the economic management of assets) Guide to the available techniques
    BS 806:1993 Specification for design and construction of ferrous piping installations for and in connection with land boilers
    PD 6539:1994 Guide to methods for the assessment of the influence of crack growth on the significance of defects in components operating at high temperatures

    Standards Referencing This Book - (Show below) - (Hide below)

    BS 5500:1997 SPECIFICATION FOR UNFIRED FUSION WELDED PRESSURE VESSELS
    • Access your standards online with a subscription

      Features

      • Simple online access to standards, technical information and regulations
      • Critical updates of standards and customisable alerts and notifications
      • Multi - user online standards collection: secure, flexibile and cost effective