AS 1580.401.6-2002
Current
The latest, up-to-date edition.
Paints and related materials - Methods of test Hard dry condition (mechanical thumb test)
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
English
13-12-2002
This Standard sets out a method for determining the hard dry condition of paint films.
Committee |
CH-003
|
DocumentType |
Standard
|
ISBN |
0 7337 4931 3
|
Pages |
4
|
ProductNote |
This standard has been reconfirmed in Australia in 2013 and remains current in New Zealand. Reconfirmation Notice 13-11-2013
|
PublisherName |
Standards Australia
|
Status |
Current
|
Supersedes |
This Standard sets out a method for determining the hard dry condition of paint films. NOTES: 1 Because of the great variety of paints and the different types of deformation, the method does not attempt to specify an end point. That has been left to the appropriate product specification.2 This test should not be undertaken until the paint film has dried beyond the surface dry condition (see AS 1580.401.1).3 The terms ‘hard dry’ has not absolute meaning. The method simulates, under controlled conditions, the effect of a thumb being pressed against a paint film while being rotated through 270°.
Originated as AS K41.401.6-1969.
Previous edition AS 1580.401.6-1992.
Fourth edition 2002.
AS 1580.101.1-1986 | Paints and related materials - Methods of test Air drying conditions |
AS/NZS 1580.401.1:1999 | Paints and related materials - Methods of test Surface dry condition (Reconfirmed 2013) |
AS 1580.401.1-1981 | Paints and related materials - Methods of test Surface dry condition |
AS 1683.15.1-2000 | Methods of test for elastomers International rubber hardness (Reconfirmed 2018) |
AS/NZS 1580.101.1:1999 | Paints and related materials - Methods of test Conditions of test - Temperature, humidity and airflow control (Reconfirmed 2013) |
AS 3730.3-2006 | Guide to the properties of paints for buildings Latex - Interior - Low gloss (Reconfirmed 2016) |
AS 3730.2-2006 | Guide to the properties of paints for buildings Latex - Interior - Semi-gloss (Reconfirmed 2016) |
AS 3730.9-2006 | Guide to the properties of paints for buildings Latex - Exterior - Semi-gloss |
AS 3730.7-2006 | Guide to the properties of paints for buildings Latex - Exterior - Flat |
AS 3730.15-2006 | Guide to the properties of paints for buildings Primer - Latex - For metallic zinc surfaces |
AS 3730.16-2006 | Guide to the properties of paints for buildings Latex - Self-priming timber finish - Exterior |
AS 3730.17-2006 | Guide to the properties of paints for buildings Primer - Wood - Latex - Interior/exterior (Reconfirmed 2016) |
AS 3730.18-2006 | Guide to the properties of paints for buildings Undercoat/sealer - Latex - Interior/exterior |
AS 3730.12-2006 | Guide to the properties of paints for buildings Latex - Interior - Gloss |
AS 3730.1-2006 | Guide to the properties of paints for buildings Latex - Interior - Flat (Reconfirmed 2016) |
AS 3730.10-2006 | Guide to the properties of paints for buildings Latex - Exterior - Gloss (Reconfirmed 2016) |
AS 3730.8-2006 | Guide to the properties of paints for buildings Latex - Exterior - Low-gloss (Reconfirmed 2016) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.