AS 1580.408.4-2004
Current
The latest, up-to-date edition.
Paints and related materials - Methods of test Adhesion (crosscut) (Reconfirmed 2019)
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
English
26-11-2004
This Standard sets out a method for assessing the adhesion of paint coatings to substrates by applying and removing pressure-sensitive adhesive tape over cuts made in the coating. The method is also applicable as a field procedure, when not under the controlled environmental conditions of AS 1580.101.1, however the temperature of the surface needs to be recorded.
Committee |
CH-003
|
DocumentType |
Standard
|
ISBN |
0 7337 6380 4
|
Pages |
5
|
ProductNote |
Reconfirmed 01/11/2019.
This standard has been reconfirmed in Australia in 2019 and remains current in New Zealand. Reconfirmed 2019. Reconfirmation Notice 01/11/2019 |
PublisherName |
Standards Australia
|
Status |
Current
|
Supersedes |
This Standard sets out a method for assessing the adhesion of paint coatings to substrates by applying and removing pressure-sensitive adhesive tape over cuts made in the coating. The method is also applicable as a field procedure, when not under the controlled environmental conditions of AS1580.101.1, however the temperature of the surface needs to be recorded. It is not applicable to soft or friable substrates.The method is not considered suitable for coatings thicker than 125µm.The method does not distinguish between high levels of adhesion for which more complex procedures are required, such as a pull-off adhesion test similar to ASTMD4541 or ISO4624.In multicoat systems, if adhesion failure occurs between coats, the adhesion of the coating system to the substrate cannot be determined.
Originated as AS 1580.408.4-1980.
Previous edition 1993.
Third edition 2004.
AS 1580.101.4-1986 | Paints and related materials - Methods of test Conditions of test, temperature controlled |
AS 1580.101.1-1986 | Paints and related materials - Methods of test Air drying conditions |
AS/NZS 1580.103.1:1995 | Paints and related materials Methods of test - Examination and preparation of samples for testing (Reconfirmed 2013) |
AS 1580.103.1-1980 | Paints and related materials - Methods of test Preliminary examination and preparation for testing |
AS/NZS 1580.107.3:1997 | Paints and related materials - Methods of test Determination of wet film thickness by gauge (Reconfirmed 2013) |
AS 1580.108.2-2004 | Paints and related materials - Methods of test Dry film thickness - Paint inspection gauge (Reconfirmed 2019) |
AS/NZS 1580.101.1:1999 | Paints and related materials - Methods of test Conditions of test - Temperature, humidity and airflow control (Reconfirmed 2013) |
AS 1580.107.3-1992 | Paints and related materials - Methods of test Determination of wet film thickness by wheel gauge |
AS/NZS 1580.108.1:1994 | Paints and related materials - Methods of test Determination of dry film thickness on metallic substrates - Non-destructive methods (Reconfirmed 2013) |
AS 1580.108.1-1980 | Paints and related materials - Methods of test Determination of dry film thickness on iron and steel substrates (permanent magnet instruments) |
AS 1580.102.1-2002 | Paints and related materials - Methods of test Sampling procedure |
AS/NZS 1580.101.4:1999 | Paints and related materials - Methods of test Conditions of test - Temperature control (Reconfirmed 2013) |
AS 1635.3.1-1993 | Methods of test for pressure-sensitive adhesive tape Adhesion strength |
AS 3730.21-2006 | Guide to the properties of paints for buildings Primer - Solvent-borne - For ferrous metallic surfaces |
AS 4647-2011 | Diaphragm gas meters |
AS 4848.1-2006 | Application specifications for coating systems Single coat inorganic (ethyl) zinc silicate - Solvent-borne |
AS/NZS 2311:2009 | Guide to the painting of buildings |
AS/NZS 3750.11:2009 | Paints for steel structures Chlorinated rubber - High-build and gloss |
AS/NZS 2130:1998 | Cots for day nursery, hospital and institutional use - Safety requirements |
AS 1580.452.1-2003 | Paints and related materials - Methods of test Resistance to humidity under condensation conditions |
AS 1627.6-2003 | Metal finishing - Preparation and pretreatment of surfaces Chemical conversion treatment of metals (Reconfirmed 2017) |
AS 3730.15-2006 | Guide to the properties of paints for buildings Primer - Latex - For metallic zinc surfaces |
AS/NZS 1580.404.1:1997 | Paints and related materials - Methods of test Recoating properties (Reconfirmed 2013) |
AS/NZS 2728:2013 | Prefinished/prepainted sheet metal products for interior/exterior building applications - Performance requirements |
AS 4506-2005 | Metal finishing - Thermoset powder coatings (Reconfirmed 2017) |
AS/NZS 3750.11:1996 | Paints for steel structures - Chlorinated rubber - High-build and gloss |
AS/NZS 3750.4:1994 | Paints for steel structures Bitumen paint (Reconfirmed 2013) |
AS/NZS 2712:2007 | Solar and heat pump water heaters - Design and construction (Reconfirmed 2020) |
AS/NZS 2312:2002 | Guide to the protection of structural steel against atmospheric corrosion by the use of protective coatings |
AS 1290.1-1995 | Linear measuring instruments used in construction - General requirements |
AS/NZS 2728:2007 | Prefinished/prepainted sheet metal products for interior/exterior building applications - Performance requirements |
AS 1580.408.2-2004 | Paints and related materials - Methods of test Adhesion - Knife test (Reconfirmed 2019) |
HB 161-2005 | Guide to Plastering |
AS/NZS 4069:2013 | Bath boards and seats - Product requirements |
AS/NZS 2280:2014 | Ductile iron pipes and fittings |
AS/NZS 3750.5:2008 | Paints for steel structures Acrylic full gloss (two-pack) (Reconfirmed 2020) |
AS/NZS 2280:2020 | Ductile iron pipes and fittings |
AS 4069-1993 | Bathseats - Product requirements |
AS/NZS 3750.20:2008 | Paints for steel structures Anticorrosive metal primer - Solvent-borne - Lead and chromate free (Reconfirmed 2020) |
AS/NZS 3973:2009 | Shower/toilet chairs (mobile and static) (Reconfirmed 2016) |
AS 3996:2019 | Access covers and grates |
AS 3715-2002 | Metal finishing - Thermoset powder coatings for architectural applications of aluminium and aluminium alloys |
AS/NZS 4443:1997 | Office panel systems - Workstations |
AS/NZS 3750.5:1994 | Paints for steel structures - Acrylic full gloss (two-pack) |
AS/NZS 3750.19:2008 | Paints for steel structures Metal primer - General purpose (Reconfirmed 2020) |
AS/NZS 2311:2017 | Guide to the Painting of Buildings |
AS 4089-1993 | Priming paint for steel - Single component - General purpose |
AS 4025.4-1994 | Paints for equipment including ships Solvent-borne - Lead and chromate free - Anticorrosive metal primer |
AS/NZS 3973:2005 | Shower/toilet chairs (mobile and static) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.