Specifies three grades of cold-rolled unalloyed low carbon steel sheet produced on a continuous mill and zinc coated by an electrolytic process. Supplied as coil or cut lengths in thicknesses from 0.3mm to 2mm and in widths from 15mm to 1250mm.
Committee |
MT-001
|
DocumentType |
Standard
|
ISBN |
0 7262 2572 X
|
Pages |
9
|
ProductNote |
Reconfirmed 27/05/2016.This standard has been reconfirmed in Australia in 2016 and remains current in New Zealand. Reconfirmation Notice 27/05/2016
|
PublisherName |
Standards Australia
|
Status |
Current
|
Supersedes |
This standard specifies requirements for cold-rolled unalloyed low carbon steel sheet and strip produced on a continuous mill and zinc-coated by an electrolytic process, supplied as coil or cut lengths in thicknesses from 0.3 mm up to and including 2.0 mm and in widths from 15 mm up to and including 1250 mm.Provision is made for three of the grades of coldrolled steel classified in terms of mechanical properties in accordance with AS 1595, produced with an exposed (E) finish, and for three classes of zinc coating according to the mass per unit area of the coating metal applied.NOTE: Guidelines to purchasers on requirements that must be specified by the purchaser and those that must be agreed at the time of enquiry and/or order are given in Appendix A.
First published 1982
AS 2505.1-2004 | Metallic materials Sheet, strip and plate - Bend tests |
AS 1213-1982 | Iron and steel - Methods of sampling |
AS/NZS 1595:1998 | Cold-rolled, unalloyed, steel sheet and strip (Reconfirmed 2016) |
AS 2338-2004 | Preferred dimensions of wrought metal products |
AS 2025.1-1977 | Method for Rockwell superficial hardness test - Testing of metals, N and T scales |
AS 1391-2007 | Metallic materials - Tensile testing at ambient temperature (Reconfirmed 2017) |
AS/NZS 1365:1996 | Tolerances for flat-rolled steel products (Reconfirmed 2016) |
AS 1815.1-2007 | Metallic materials - Rockwell hardness test Test method (scales A, B, C, D, E, F, G, H, K, N, T) (Reconfirmed 2017) |
AS 1650-1989 | Hot-dipped galvanized coatings on ferrous articles |
AS 4647-2005 | Domestic diaphragm gas meters |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.