ASTM A 269/A269M : 2015 : REV A : R2019
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service
Hardcopy , PDF
14-03-2024
English
19-09-2019
Committee |
A 01
|
DocumentType |
Standard
|
Pages |
7
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1This specification covers grades of nominal-wall-thickness, stainless steel tubing for general corrosion-resisting and low- or high-temperature service, as designated in Table 1.
Grade | Composition, % | ||||||||||||||
TP | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | |
UNS DesignationA | S24000 | S31254 | S31266 | S31725 | S31726 | S31727 | S32053 | S30600A | S32654 | S34565 | S35045 | N08367 | N08925 | N08926 | N08904 |
Carbon | 0.08 | 0.020 | 0.030 | 0.035 | 0.035 | 0.030 | 0.030 | 0.018 | 0.020 | 0.030 | 0.06– | 0.030 | 0.020 | 0.020 | 0.020 |
Manganese | 11.5– | 1.00 | 2.00–4.00 | 2.00 | 2.00 | 1.00 | 1.00 | 2.0 | 2.0– | 5.0– | 1.50 | 2.00 | 1.00 | 2.00 | 2.00 |
Phosphorus | 0.060 | 0.030 | 0.035 | 0.045 | 0.045 | 0.030 | 0.030 | 0.020 | 0.030 | 0.030 | 0.045 | 0.040 | 0.045 | 0.030 | 0.040 |
Sulfur. | 0.030 | 0.015 | 0.020 | 0.030 | 0.030 | 0.030 | 0.010 | 0.020 | 0.005 | 0.010 | 0.015 | 0.030 | 0.030 | 0.010 | 0.030 |
Silicon | 1.00 | 0.80 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 3.7–4.3 | 0.50 | 1.00 | 1.00 | 1.00 | 0.50 | 0.50 | 1.00 |
Nickel | 2.3– | 17.5– | 21.0–24.0 | 13.5– | 14.5– | 14.5– | 24.0– | 14.0– | 21.0– | 16.0– | 32.0– | 23.5– | 24.0–26.0 | 24.0– | 23.0– |
Chromium | 17.0– | 19.5– | 23.0–25.0 | 18.0– | 17.0– | 17.5– | 22.0– | 17.0– | 24.0– | 23.0– | 25.0– | 20.0– | 19.0–21.0 | 19.0– | 19.0– |
Molybdenum | ... | 6.0– | 5.2–6.2 | 4.0– | 4.0– | 3.8– | 5.0– | 0.20 | 7.0– | 4.0– | 6.0– | 6.0–7.0 | 6.0– | 4.0– | |
Titanium | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | 0.15– | . . . | . . . | . . . | . . . |
Columbium | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | 0.10 | . . . | . . . | . . . | . . . | . . . |
Tantalum | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | ||
NitrogenF | 0.20– | 0.18– | 0.35–0.60 | 0.20 | 0.10– | 0.15– | 0.17– | 0.45– | 0.40– | . . . | 0.18– | 0.10–0.20 | 0.15– | 0.10 | |
Vanadium | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | . . . | |||||
Copper | . . . | 0.50– | 1.00–2.50 | . . . | . . . | 2.8– | . . . | 0.50 | 0.30– | . . . | 0.75 | 0.75 | 0.80–1.50 | 0.50– | 1.00– |
Others | . . . | . . . | W 1.50–2.50 | . . . | . . . | . . . | . . . | . . . | . . . | . . . | Al | . . . | . . . | . . . | . . . |
1.2The tubing sizes and thicknesses usually furnished to this specification are 1/4in. [6.4 mm] in inside diameter and larger and 0.020 in. [0.51 mm] in nominal wall-thickness and heavier.
1.3Mechanical property requirements do not apply to tubing smaller than 1/8in. [3.2 mm] in inside diameter or 0.015 in. [0.38 mm] in thickness.
Note 1:Additional testing requirements may apply for use in ASME B31.3 applications.
1.4Optional supplementary requirements are provided and, when one or more of these are desired, each shall be so stated in the order.
1.5The values stated in either SI units or inch-pound units are to be regarded separately as standard. Within the text, SI units are shown in brackets. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. The inch-pound units shall apply unless the “M” designation of this specification is specified in the order.
1.6This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
ASTM F 3347 : 2022 | Standard Specification for Metal Press Insert Fittings with Factory Assembled Stainless Steel Press Sleeve for SDR9 Cross-linked Polyethylene (PEX) Tubing and SDR9 Polyethylene of Raised Temperature (PE-RT) Tubing |
ASTM C 852/C852M : 2017 : R2022 | Standard Guide for Design Criteria for Plutonium Gloveboxes |
ASTM F 2854 : 2021 | Standard Specification for Push-Fit Crosslinked Polyethylene (PEX) Mechanical Fittings for Crosslinked Polyethylene (PEX) Tubing |
ASTM F 2929 : 2017 : R2021 | Standard Specification for Crosslinked Polyethylene (PEX) Tubing of 0.070 in. Wall and Fittings for Radiant Heating Systems up to 75 psig |
ASTM A 1119/A1119M : 2022 | Standard Specification for Welded Partially Corrugated Tube for Potable Water and General Service |
ASTM F 3348 : 2022 | Standard Specification for Plastic Press Insert Fittings with Factory Assembled Stainless Steel Press Sleeve for SDR9 Cross-linked Polyethylene (PEX) Tubing and SDR9 Polyethylene of Raised Temperature (PE-RT) Tubing |
ASTM E 2181/E2181M : 2019 | Standard Specification for Compacted Mineral-Insulated, Metal-Sheathed, Noble Metal Thermocouples and Thermocouple Cable |
ASTM A 1016/A1016M : 2002 | Standard Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes |
ASTM A 480/A480M : 2022 | Standard Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip |
ASTM A 262 : 2001 | Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels |
ASTM A 632 : 1998 | Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service |
ASTM A 262 : 1998 | Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels |
ASTM A 262 : 2015 | Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels |
ASTM A 480/A480M : 2020 : REV A | Standard Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip |
ASTM A 480/A480M : 2022 : REV A | Standard Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip |
ASTM A 262 : 2015 : R2021 | Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.