ASTM A 518/A518M : 1999 : R2008
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Corrosion-Resistant High-Silicon Iron Castings
Hardcopy , PDF
11-11-2014
English
01-10-2008
CONTAINED IN VOL. 01.02, 2017 Defines high-silicon cast iron castings intended for corrosion-resistant service.
Committee |
A 04
|
DevelopmentNote |
Supersedes ASTM A 518 (04/04)
|
DocumentType |
Standard
|
Pages |
6
|
ProductNote |
Reconfirmed 2008
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This specification covers high-silicon cast iron castings intended for corrosion-resistant service.
1.2 This specification covers three grades as shown in Table 1. Selection of grade depends on the corrosive service to be experienced by the casting. All three grades are suited for application in severe corrosive environments. However, Grade 2 is particularly suited for application in strong chloride environments, and Grade 3 is recommended for impressed current anodes.
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.4 The following safety hazards caveat pertains only to the test method portion, Section 9, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Element | Composition, Weight % | ||
---|---|---|---|
Grade 1 | Grade 2 | Grade 3 | |
Carbon | 0.65–1.10 | 0.75–1.15 | 0.70–1.10 |
Manganese | 1.50, max | 1.50, max | 1.50, max |
Silicon | 14.20–14.75 | 14.20–14.75 | 14.20–14.75 |
Chromium | 0.50, max | 3.25–5.00 | 3.25–5.00 |
Molybdenum | 0.50, max | 0.40–0.60 | 0.20, max |
Copper | 0.50, max | 0.50, max | 0.50, max |
ASTM E 350 : 2012-09 | TEST METHODS FOR CHEMICAL ANALYSIS OF CARBON STEEL, LOW-ALLOY STEEL, SILICON ELECTRICAL STEEL, INGOT IRON, AND WROUGHT IRON |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.