• Shopping Cart
    There are no items in your cart

ASTM A 599/A599M : 2007 : R2017

Current

Current

The latest, up-to-date edition.

Standard Specification for Tin Mill Products, Electrolytic Tin-Coated, Cold-Rolled Sheet

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

25-09-2017

€49.35
Excluding VAT

This specification covers cold-rolled steel sheet in coils or in cut lengths, tin-coated by electrodeposition.

Committee
A 01
DevelopmentNote
Supersedes ASTM A 599. (05/2002)
DocumentType
Standard
Pages
3
ProductNote
Reconfirmed 2017
PublisherName
American Society for Testing and Materials
Status
Current
Supersedes

1.1This specification covers cold-rolled steel sheet in coils or in cut lengths, tin-coated by electrodeposition. The product is commonly known as electrolytic tin-coated sheet, and is for applications that need good solderability, good surface appearance, and a degree of corrosion resistance. Tin-coated sheet is produced to various designations of tin coating, as outlined in Table 1.

TABLE 1 Electrolytic Tin-Coated Sheets Coating Weight [Mass]

Note 1:Listed below are the commonly produced coating weights [mass] upon agreement between the producer and the purchaser. Other combinations of coatings may be specified and the appropriate minimum average test valuesA apply.

Designation No.

Nominal Tin Coating
Weight [Mass]
(Each Surface)
lb/base box (g/m2)B

Minimum Average Coating
Weight [Mass]
(Each Surface Test Value)
lb/base box (g/m2)B, C

5 (0.6/0.6)

0.025/0.025 (0.6/0.6)

0.02/0.02 (0.5/0.5)

10 (1.1/1.1) 

0.05/0.05 (1.1/1.1)

0.04/0.04 (0.9/0.9)

15 (1.7/1.7) 

0.075/0.075 (1.7/1.7)

0.06/0.06 (1.4/1.4)

20 (2.2/2.2) 

0.10/0.10 (2.2/2.2)

0.08/0.08 (1.8/1.8)

25 (2.8/2.8) 

0.125/0.125 (2.8/2.8)

0.11/0.11 (2.5/2.5)

50 (5.6/5.6) 

0.25/0.25 (5.6/5.6)

0.23/0.23 (5.2/5.2)

75 (8.4/8.4) 

0.375/0.375 (8.4/8.4)

0.35/0.35 (7.8/7.8)

100 (11.2/11.2)

0.50/0.50 (11.2/11.2)

0.45/0.45 (10.1/10.1)

(A)Refer to Specifications A623 and A623M.
(B)A base box is defined as a unit of area equivalent to 112 sheets 14 in. by 20 in. or 31 360 in.2  (refer to Specification A623).
(C)The minimum single spot value shall not be less than 80 % of the minimum average tin coating weight [mass] (see 8.1 and 8.2).

1.1.1Electrolytic tin-coated sheet is customarily available as commercial steel (CS); drawing steel (DS); deep drawing steel (DDS); extra deep drawing steel (EDDS), and structural steel (SS). The tin coating is available as unmelted or melted.

1.2Limitations—This specification is applicable to orders in either inch-pound units (as A599), which is supplied in thicknesses from 0.015 in. to 0.036 in., or SI units [as A599M], which is supplied in thicknesses from 0.381 mm to 0.914 mm. For thicknesses lighter than 0.015 in. [0.381 mm], refer to A624/A624M [A624M].

1.3Unless the order shows the “M” designation [SI units], the product shall be furnished to inch-pound units. The values stated in either inch-pound or SI units are to be regarded as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with this specification.

1.4This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

ASTM A 754/A754M : 2018 Standard Test Method for Coating Weight (Mass) of Metallic Coatings on Steel by X-Ray Fluorescence
ASTM A 987/A987M : 2019 Standard Practice for Measuring Shape Characteristics of Tin Mill Products

ASTM A 624/A624M : 2013 : R2018 Standard Specification for Tin Mill Products, Electrolytic Tin Plate, Single Reduced
ASTM A 1008/A1008M : 2020 Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 623 : 2022 Standard Specification for Tin Mill Products, General Requirements
ASTM A 630 : 2016 : REV A : EDT 1 Standard Test Methods for Determination of Tin Coating Weights for Electrolytic Tin Plate
ASTM A 623M : 2016 : REDLINE Standard Specification for Tin Mill Products, General Requirements [Metric]
ASTM A 1008/A1008M : 2016-09 SPECIFICATION FOR STEEL, SHEET, COLD-ROLLED, CARBON, STRUCTURAL, HIGH-STRENGTH LOW-ALLOY, HIGH-STRENGTH LOW-ALLOY WITH IMPROVED FORMABILITY, SOLUTION HARDENED, AND BAKE HARDENABLE
ASTM A 624/A624M : 2022 Standard Specification for Tin Mill Products, Electrolytic Tin Plate, Single Reduced
ASTM A 1008/A1008M : 2021 Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 623M : 2016 Standard Specification for Tin Mill Products, General Requirements [Metric]
ASTM A 623 : 2016 : REDLINE Standard Specification for Tin Mill Products, General Requirements
ASTM A 630 : 2016 : REV A : R2024 Standard Test Methods for Determination of Tin Coating Weights for Electrolytic Tin Plate
ASTM A 1008/A1008M : 2021 : REV A Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 1008/A1008M : 2023 : EDT 1 Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 1008/A1008M : 2024 Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 700 : 2014 Standard Guide for Packaging, Marking, and Loading Methods for Steel Products for Shipment
ASTM A 623 : 2016 Standard Specification for Tin Mill Products, General Requirements
ASTM A 1008/A1008M : 2023 Standard Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, Required Hardness, Solution Hardened, and Bake Hardenable
ASTM A 623M : 2022 Standard Specification for Tin Mill Products, General Requirements [Metric]

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.