ASTM A 626/A626M : 2016 : REDLINE
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Tin Mill Products, Electrolytic Tin Plate, Double Reduced
24-03-2022
English
15-12-2016
CONTAINED IN VOL. 01.06, 2017 Defines double-reduced electrolytic tin plate produced from low-carbon cold-reduced steel furnished in coils and cut sizes for use predominately in the manufacture of cans.
Committee |
A 01
|
DevelopmentNote |
Supersedes ASTM A 626 (04/04)
|
DocumentType |
Redline
|
Pages |
5
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy |
1.1This specification covers double-reduced electrolytic tin plate produced from low-carbon cold-reduced steel furnished in coils and cut sizes for use predominately in the manufacture of cans. It is furnished in commercially available tin coating weights [masses] and is normally supplied with a trimmed edge.
1.2This specification is applicable to orders in either inch-pound units (as A626) which is supplied in thicknesses from 0.0050 to 0.0118 in. or SI units [as A626M] which is supplied in thicknesses from 0.127 to 0.300 mm.
1.3The values stated in either inch-pound or SI units are to be regarded as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents. Therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with this specification.
1.4This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
ASTM A 987/A987M : 2009 | Standard Practice for Measuring Shape Characteristics of Tin Mill Products |
MIL-DTL-2439 Revision G:2014 | CONTAINER, AMMUNITION, FIBER, SPIRALLY WOUND |
ASTM A 987/A987M : 2009 : R2014 | Standard Practice for Measuring Shape Characteristics of Tin Mill Products |
ASTM A 623M : 2016 : REDLINE | Standard Specification for Tin Mill Products, General Requirements [Metric] |
ASTM B 339 : 2012 : REDLINE | Standard Specification for Pig Tin |
ASTM A 623 : 2016 : REDLINE | Standard Specification for Tin Mill Products, General Requirements |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.