ASTM A 834 : 1995 : R2011
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Common Requirements for Iron Castings for General Industrial Use
Hardcopy , PDF
11-11-2014
English
01-03-2011
CONTAINED IN VOL. 01.02, 2017 Defines requirements used in conjunction with iron casting specifications issued by ASTM.
Committee |
A 04
|
DocumentType |
Standard
|
Pages |
4
|
ProductNote |
Reconfirmed 2011
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This specification covers a group of requirements that are mandatory requirements when used in conjunction with the following iron casting specifications issued by ASTM:
ASTM Specification2 |
A47/A47M |
A48/A48M |
A197/A197M |
A220/A220M |
A278/A278M |
A319 |
A395/A395M |
A436 |
A439 |
A518/A518M |
A532/A532M |
A536 |
A571/A571M |
A823 |
A842 |
A874/A874M |
A897/A897M |
1.2 This specification also covers a group of supplementary requirements which may be applied to the above specifications as indicated herein. These are provided for use when additional testing or inspection is desired and apply only when specified individually by the purchaser in the order.
1.3 The requirements of the individual material specification, and this general specification shall prevail in the sequence named.
1.4 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.
ASTM A 518/A518M : 1999 | Standard Specification for Corrosion-Resistant High-Silicon Iron Castings |
ASTM E 689 : 2015 : REDLINE | Standard Reference Radiographs for Ductile Iron Castings |
MIL-STD-129 Revision R:2014 | Military Marking for Shipment and Storage |
ASTM A 47/A47M : 1999 | Standard Specification for Ferritic Malleable Iron Castings |
ASTM E 802 : 2015 : REDLINE | Standard Reference Radiographs for Gray Iron Castings Up to 4<fraction><num>1</num><den>2</den> </fraction> in. (114 mm) in Thickness |
ASTM A 395/A395M : 1999 | Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures |
ASTM A 897/A897M : 2016 : REDLINE | Standard Specification for Austempered Ductile Iron Castings |
ASTM E 10 : 2017-05 | TEST METHOD FOR BRINELL HARDNESS OF METALLIC MATERIALS |
ASTM E 30 : 1989 | Test Methods for Chemical Analysis of Steel, Cast Iron, Open-Hearth Iron, and Wrought Iron (Withdrawn 1995) |
FED-STD-123 Revision H:2007 | MARKING FOR SHIPMENT (CIVIL AGENCIES) |
ASTM E 8 : 2004 | Standard Test Methods for Tension Testing of Metallic Materials |
ASTM E 709 : 2015 : REDLINE | Standard Guide for Magnetic Particle Testing |
ASTM A 644 : 2017 : REDLINE | Standard Terminology Relating to Iron Castings |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.