Standard Specification for Fusion Bonded Epoxy-Coated Pipe Piles
Hardcopy , PDF
11-11-2014
English
10-03-2000
CONTAINED IN VOL. 01.01, 2017 Deals with pipe piles with fusion-bonded epoxy powder protective coating which is applied by electrostatic flocking, spray or fluidized bed process.
Committee |
A 01
|
DevelopmentNote |
Supersedes ASTM A 972 (04/04)
|
DocumentType |
Standard
|
Pages |
4
|
ProductNote |
Reconfirmed 2000
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy |
1.1 This specification covers pipe piles with protective fusion-bonded epoxy powder coating applied by the electrostatic spray, flocking , or fludized bed process.
Note 1-The coating applicator is identified throughout this specification as the manufacturer.
1.2 Other organic coatings may be used provided they meet the requirements of this specification.
1.3 Requirements for the powder coating are contained in Annex A1.
1.4 This specification is applicable for orders in either SI units (as Specification A 972M) or inch-pound units (as Specification A 972). The values stated in either SI or inch-pound units are to be regarded as standard. Within the text, the inch-pound units are shown in brackets.
1.5 The following precautionary statement refers to the test method portion only, Section 8, of this standard: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
API 5L7 : 1988(R2015) | RECOMMENDED PRACTICE FOR UNPRIMED INTERNAL FUSION BONDED EPOXY COATING OF LINE PIPE |
ASTM G 8 : 1996 | Standard Test Methods for Cathodic Disbonding of Pipeline Coatings |
NACE TM 01 1975 : 1975 | VISUAL COMPARATOR FOR SURFACES OF NEW STEEL CENTRIFUGALLY BLAST CLEANED WITH STEEL GRIT AND SHOT |
NACE RP 04 90 : 0 | HOLIDAY DETECTION OF FUSION-BONDED EPOXY EXTERNAL PIPELINE COATINGS OF 250 TO 760 MICRON (10 TO 30 MILS) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.