ASTM B 135/B135M : 2017
Current
The latest, up-to-date edition.
Standard Specification for Seamless Brass Tube
Hardcopy , PDF
English
01-10-2017
CONTAINED IN VOL. 02.01, 2017 Defines seamless round and rectangular including square copper alloy tube in straight lengths.
Committee |
B 05
|
DevelopmentNote |
Supersedes ASTM B 135 & ASTM B 135M. (11/2017)
|
DocumentType |
Standard
|
Pages |
8
|
PublisherName |
American Society for Testing and Materials
|
Status |
Current
|
Supersedes |
1.1This specification covers seamless round and rectangular including square copper alloy tube in straight lengths. Ten alloys are specified having the following nominal compositions:
Copper | Previously | Nominal Composition, % | |||
Alloy | Used | ||||
UNS No.2 | DesignationA | Copper | Zinc | Lead | Tin |
| |||||
C22000 | 7 | 90.0 | 10.0 | ... | ... |
C23000 | 1 | 85.0 | 15.0 | ... | ... |
C26000 | 2 | 70.0 | 30.0 | ... | ... |
C27000 | 9 | 65.0 | 35.0 | ... | ... |
C27200 | 8 | 63.0 | 37.0 | ... | ... |
C27400 | ... | 62.5 | 37.5 | ... | ... |
C28000 | 5 | 60.0 | 40.0 | ... | ... |
C33000 | 3 | 66.0 | 33.5 | 0.5 | ... |
C33200 | 4 | 66.0 | 32.4 | 1.6 | ... |
C37000 | 6 | 60.0 | 39.0 | 1.0 | ... |
C44300 | ... | 71.5 | 27.5 | ... | 1.00 |
1.2The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.3Warning—Mercury has been designated by many regulatory agencies as a hazardous substance that can cause serious medical issues. Mercury, or its vapor, has been demonstrated to be hazardous to health and corrosive to materials. Caution should be taken when handling mercury and mercury containing products. See the applicable product Safety Data Sheet (SDS) for additional information. Users should be aware that selling mercury and/or mercury containing products into your state or country may be prohibited by law. (See 10.1.)2
1.4This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.5This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
ASTM B 858 : 2006 : R2018 | Standard Test Method for Ammonia Vapor Test for Determining Susceptibility to Stress Corrosion Cracking in Copper Alloys |
ASTM B 858 : 2006 : R2024 | Standard Test Method for Ammonia Vapor Test for Determining Susceptibility to Stress Corrosion Cracking in Copper Alloys |
ASTM B 846 : 2019 : REV A | Standard Terminology for Copper and Copper Alloys |
ASTM B 968/B968M : 2016 | Standard Test Method for Flattening of Copper and Copper-Alloy Pipe and Tube |
ASTM E 243 : 2018 | Standard Practice for Electromagnetic (Eddy Current) Examination of Copper and Copper-Alloy Tubes |
ASTM B 154 : 2016 | Standard Test Method for Mercurous Nitrate Test for Copper Alloys |
ASTM B 846 : 2024 | Standard Terminology for Copper and Copper Alloys |
ASTM E 527 : 2023 | Standard Practice for Numbering Metals and Alloys in the Unified Numbering System (UNS) |
ASTM E 527 : 2016 | Standard Practice for Numbering Metals and Alloys in the Unified Numbering System (UNS) |
ASTM E 243 : 2024 | Standard Practice for Electromagnetic (Eddy Current) Examination of Copper and Copper-Alloy Tubes |
ASTM B 153 : 2022 | Standard Test Method for Expansion (Pin Test) of Copper and Copper-Alloy Pipe and Tubing |
ASTM B 968/B968M : 2016 : R2022 | Standard Test Method for Flattening of Copper and Copper-Alloy Pipe and Tube |
ASTM B 153 : 2011 : R2017 | Standard Test Method for Expansion (Pin Test) of Copper and Copper-Alloy Pipe and Tubing |
ASTM B 601 : 2024 | Standard Classification for Temper Designations for Copper and Copper Alloys—Wrought and Cast |
ASTM B 601 : 2018 : REV A | Standard Classification for Temper Designations for Copper and Copper Alloys—Wrought and Cast |
ASTM B 154 : 2016 : R2022 | Standard Test Method for Mercurous Nitrate Test for Copper Alloys |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.