Standard Guide for Preparation of High-Carbon Steel for Electroplating
Hardcopy , PDF
English
03-12-2020
Committee |
B 08
|
DocumentType |
Guide
|
Pages |
5
|
PublisherName |
American Society for Testing and Materials
|
Status |
Current
|
Supersedes |
1.1This guide is intended as an aid in establishing and maintaining a preparatory cycle for electroplating on high-carbon steel (Note 1) producing a minimum of hydrogen embrittlement and maximum adhesion of the electrodeposited metal. For the purpose of this guide, steels containing 0.35 % of carbon or more, and case-hardened low-carbon steel, are defined as high-carbon steels. There is no generally recognized definite carbon content dividing high from low-carbon steels for electroplating purposes.
Note 1:Electroplating of plain high-carbon steel introduced problems not found in similar operations on low-carbon steel. During the cleaning and electroplating cycle, high-carbon steel differs from low-carbon steel in regard to its greater tendency to become embrittled and the greater difficulty in obtaining maximum adhesion of the electrodeposit. The preparation of low-carbon steel for electroplating is covered in Practice B183.
1.2This guide does not apply to the electroplating of alloy steel. For methods of chromium electroplating directly on steel, see Guide B177.
1.3The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. For a specific hazards statement, see 3.1.
1.5This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
SAE AMS2428A | Plating, Cobalt-Phosphorus, Nanocrystalline |
ASTM B 183 : 2018 : R2022 | Standard Practice for Preparation of Low-Carbon Steel for Electroplating |
ASTM B 850 : 1998 : R2022 | Standard Guide for Post-Coating Treatments of Steel for Reducing the Risk of Hydrogen Embrittlement |
ASTM B 850 : 1998 : R2015 | Standard Guide for Post-Coating Treatments of Steel for Reducing the Risk of Hydrogen Embrittlement |
ASTM B 849 : 2002 : R2023 | Standard Specification for Pre-Treatments of Iron or Steel for Reducing Risk of Hydrogen Embrittlement |
ASTM B 849 : 2002 : R2019 | Standard Specification for Pre-Treatments of Iron or Steel for Reducing Risk of Hydrogen Embrittlement |
ASTM B 183 : 2018 | Standard Practice for Preparation of Low-Carbon Steel for Electroplating |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.