1.1This specification2 covers forgings of:

Alloy Type

UNS Number(s)

Fe-Ni-Cr-Mo-N

N08367

Low-carbon Cr-Ni-Fe-N

R20033

Low-carbon Ni-Cr-Mo

N06035, N06058, N06059, N06044

Low-carbon Ni-Cr-Mo-Cu

N06200

Low-carbon Ni-Cr-Mo-W

N06686

Low-carbon Ni-Fe-Cr-Mo-Cu

N08031, N08034

Low-carbon Ni-Mo-Cr

N10276, N06022, N10362

Low-carbon Ni-Mo-Cr-Ta

N06210

Ni

N02200

Ni-Co-Cr-Si

N12160

Ni-Cr-Al

N06699

Ni-Cr-Co-Mo

N06617

Ni-Cr-Fe

N06600, N06603, N06690

Ni-Cr-Fe-Al

N06025

Ni-Cr-Fe-Si

N06045

Ni-Cr-Mo-Nb

N06625

Ni-Cr-Mo-Si

N06219

Ni-Cr-Mo-W

N06110

Ni-Cr-W-Mo

N06230

Ni-Cu

N04400

Ni-Fe-Cr

N08120, N08800, N08810, N08811

Ni-Fe-Cr-Mo-Cu

N08825, N08827

Ni-Fe-Cr-W

N06674

Ni-Mo

N10665, N10675, N10629

Ni-Mo-Cr-Fe

N10242, N10624

1.1.1The nickel-iron-chromium alloys are UNS N08120, UNS N08800, UNS N08810, and UNS N08811. Alloy UNS N08800 is normally employed in service temperatures up to and including 1100 °F (593 °C). Alloys UNS N08810, N08120, and UNS N08811 are normally employed in service temperatures above 1100 °F (593 °C) where resistance to creep and rupture is required, and are annealed to develop controlled grain size for optimum properties in this temperature range.

1.1.2Nickel-iron-chromium-tungsten alloy UNS N06674 is normally employed in service temperatures above 1100 °F (593 °C) where resistance to creep and rupture is required, and is annealed to develop optimum properties in this temperature range.

1.1.3Nickel-chromium-molybdenum-columbium (UNS N06625) products are furnished in two grades of different heat-treated conditions:

1.1.3.1Grade 1 (Annealed)—Material is normally employed in service temperatures up to 1100 °F (593 °C).

1.1.3.2Grade 2 (Solution annealed)—Material is normally employed in service temperatures above 1100 °F (593 °C) where resistance to creep and rupture are required.

Note 1:Hot-working or reannealing may change properties significantly, depending on working history and temperatures.

1.2The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.3This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Safety Data Sheet (SDS) for this product/material as provided by the manufacturer, to establish appropriate safety, health, and environmental practices, and determine the applicability of regulatory limitations prior to use.

1.4This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

ASTM F 1387 : 2019 Standard Specification for Performance of Piping and Tubing Mechanically Attached Fittings
ASTM B 366/B366M : 2020 Standard Specification for Factory-Made Wrought Nickel and Nickel Alloy Fittings

ASTM E 8/E8M : 2024 Standard Test Methods for Tension Testing of Metallic Materials
ASTM B 880 : 2014 : R2019 Standard Specification for General Requirements for Chemical Check Analysis Limits for Nickel, Nickel Alloys and Cobalt Alloys
ASTM E 8/E8M : 2021 Standard Test Methods for Tension Testing of Metallic Materials
ASTM B 880 : 2024 Standard Specification for General Requirements for Chemical Check Analysis Limits for Nickel, Nickel Alloys and Cobalt Alloys
ASTM E 1473 : 2022 Standard Test Methods for Chemical Analysis of Nickel, Cobalt, and High-Temperature Alloys
ASTM E 8/E8M : 2022 Standard Test Methods for Tension Testing of Metallic Materials
ASTM E 350 : 2023 Standard Test Methods for Chemical Analysis of Carbon Steel, Low-Alloy Steel, Silicon Electrical Steel, Ingot Iron, and Wrought Iron
ASTM E 350 : 2018 Standard Test Methods for Chemical Analysis of Carbon Steel, Low-Alloy Steel, Silicon Electrical Steel, Ingot Iron, and Wrought Iron
ASTM E 1473 : 2016 Standard Test Methods for Chemical Analysis of Nickel, Cobalt and High-Temperature Alloys
ASTM E 112 : 2013 : R2021 Standard Test Methods for Determining Average Grain Size
ASTM E 112 : 2024 Standard Test Methods for Determining Average Grain Size

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.