ASTM B 591 : 2004
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Copper-Zinc-Tin and Copper-Zinc-Tin-Iron-Nickel Alloys Plate, Sheet, Strip, and Rolled Bar
Hardcopy , PDF
11-11-2014
English
01-10-2004
Committee |
B 05
|
DocumentType |
Standard
|
Pages |
6
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This specification covers the requirements for specified copper-zinc-tin alloys and copper-zinc-tin-iron-nickel alloys in the form of plate, sheet, strip, and rolled bar. The alloys and nominal compositions are as follows:
Copper Alloy UNS No. | Copper, % | Tin, % | Zinc, % | Phos., %% | Iron, % | Nickel, % |
C40500 | 95 | 1 | 4 | |||
C40810 | 95.5 | 2.0 | 2.22 | 0.03 | 0.1 | 0.15 |
C40850 | 95.5 | 3.0 | 1.27 | 0.1 | 0.1 | 0.1 |
C40860 | 94.8 | 2.0 | 3.04 | 0.03 | 0.03 | 0.1 |
C41100 | 91 | 0.5 | 8.5 | |||
C41300 | 91 | 1 | 8 | |||
C41500 | 91 | 2 | 7 | |||
C42200 | 87 | 1 | 12 | |||
C42500 | 88 | 2 | 10 | |||
C42520 | 89.8 | 2.0 | 7.970.1 | 0.1 | 0.1 | |
C43000 | 85 | 2 | 13 | |||
C43400 | 85 | 0.7 | 14.3 |
1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.