• There are no items in your cart

ASTM B 792 : 2008

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Standard Specification for Zinc Alloys in Ingot Form for Slush Casting

Available format(s)

Hardcopy , PDF

Superseded date

11-11-2014

Language(s)

English

Published date

01-11-2008

Committee
B 02
DocumentType
Standard
Pages
3
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1 This specification covers commercial zinc alloys in ingot form for remelting for the manufacture of castings from the alloys as specified and designated as shown in Table 1.

1.2 Slush casting alloys are used primarily for the manufacture of hollow castings such as lighting fixtures, lamp bases, and small statues.

1.3 This specification covers two zinc alloys which are specified and designated as follows:

UNSASTM
Z34510Slush Casting Alloy A
Z30500Slush Casting Alloy B

1.4 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.

TABLE 1 Chemical and North American Color Code RequirementsA,B

Composition, %
UNS Z34510
Slush Casting Alloy A
UNS Z30500
Slush Casting Alloy B
Color CodeCBlack/RedBlack/Orange
Element
Copper 0.20.3 0.1 max
Aluminum4.505.00 5.255.75
Lead 0.007 max0.007 max
Cadmium 0.005 max0.005 max
Tin 0.005 max0.005 max
Iron 0.100 max0.100 max
Magnesium0.010 max0.010 max
Zinc RemainderRemainder

A The following applies to all specified limits in this table. For purposes of determining conformance with this specification, the observed or calculated value obtained from analysis shall be rounded off to the nearest unit in the last right-hand place of figures used in expressing the specified limit, in accordance with the rounding method of Practice E 29.

B UNS designations were established in accordance with Practice E 527.

C Refer to Practice B 908. (Note: Colors indicated are for North American applications.)

€60.48
Excluding VAT

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.