Standard Specification for Zinc Master Alloys for Use in Hot Dip Galvanizing

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

15-04-2009

Committee
B 02
DocumentType
Standard
Pages
3
PublisherName
American Society for Testing and Materials
Status
NA
SupersededBy
Supersedes

1.1 This specification covers zinc master alloys which are used in hot dip galvanizing for the purpose of adjusting the concentration of certain alloying elements in the molten zinc bath. Table 1 covers the chemical composition of these materials which include six master alloys of zinc-aluminum (brightener) and one master alloy of zinc-antimony.

ASTM Common UNS
Type A-190/10 Zn/Al High PurityZ30750
Type A-290/10 Zn/Al Low PurityZ31710
Type A-395/5 Zn/Al High PurityZ30503
Type A-495/5 Zn/Al Low PurityZ31510
Type A-596/4 Zn/Al High Purity...
Type A-696/4 Zn/AlLow Purity...
Type S-190/10 Zn/Sb Z55710

1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.

TABLE 1 Chemical Requirements Composition, % (Range or Maximum Value)A

Type A-190 % Zinc10 % Aluminum (90/10 Zn/Al)High Purity
Type A-290 % Zinc10 % Aluminum (90/10 Zn/Al)Low Purity
Type A-395 % Zinc5 % Aluminum (95/5 Zn/Al)High Purity
Type A-495 % Zinc5 % Aluminum (95/5 Zn/Al)Low Purity
Type A-596 % Zinc4 % Aluminum (96/4 Zn/Al)High Purity
Type A-696 % Zinc4 % Aluminum (96/4 Zn/Al)Low Purity
Type S-190 % Zinc10 % Antimony (90/10 Zn/Sb)
UNSBType A-1
90/10 Zn/Al
Z30750
Type A-2
90/10 Zn/Al
Z31710
Type A-3
95/5 Zn/Al
Z30503
Type A-4
95/5 Zn/Al
Z31510
Type A-5
96/4 Zn/Al
ZXXXXX
Type A-6
96/4 Zn/Al
ZXXXXX
Type S-1
90/10 Zn/Sb
Z55710
Fe0.05 max0.15 max0.05 max0.15 max0.05 max0.15 max0.03 max
Pb0.005 max0.4 max0.005 max0.4 max0.0005 max0.4 max0.015 max
Cd0.004 max...0.004 max...0.004 max...0.003 max
Cu0.035 max0.5 max0.035 max0.5 max0.035 max0.5 max0.003 max
Mg............0.06 max0.06 max
Sn0.003 max...0.003 max...0.003 max...0.01 max
As..................0.015 max
Al9.510.59.510.54.55.54.55.54.0-4.54.0-4.5...
SbC..................9.510.5
Others, Total0.01 max0.25 max0.01 max0.25 max0.01 max0.25 max0.03 max
ZnDRemainderRemainderRemainderRemainderRemainderRemainderRemainder

A The following applies to all specified limits in this table: For purposes of determining conformance with this specification, an observed value obtained from analysis shall be rounded off to the nearest unit in the last right-hand place of figures used in expressing the limiting value, in accordance with the rounding method of Practice E 29.

B UNS numbers in conformance with Practice E 527.

C Chemical method under development.

D For information only. Quantitative determination of this element is not required. Zinc is assumed to be the difference between 100 % and the sum of those elements listed above.

€60.48
Excluding VAT

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.