This specification covers titanium and titanium alloy wire as follows.

Committee
B 10
DocumentType
Standard
Pages
7
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1This specification covers titanium and titanium alloy wire as follows:

1.1.1Grade 1—UNS R50250. Unalloyed titanium,

1.1.2Grade 2—UNS R50400. Unalloyed titanium,

1.1.2.1Grade 2H—UNS R50400. Unalloyed titanium (Grade 2 with 58 ksi (400 MPa) minimum UTS),

1.1.3Grade 3—UNS R50550. Unalloyed titanium,

1.1.4Grade 4—UNS R50700. Unalloyed titanium,

1.1.5Grade 5—UNS R56400. Titanium alloy (6 % aluminum, 4 % vanadium),

1.1.6Grade 6—UNS R54520. Titanium alloy (5 % aluminum, 2.5 % tin),

1.1.7Grade 7—UNS R52400. Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.7.1Grade 7H—UNS R52400. Unalloyed titanium plus 0.12 to 0.25 % palladium (Grade 7 with 58 ksi (400 MPa) minimum UTS),

1.1.8Grade 9—UNS R56320. Titanium alloy (3 % aluminum, 2.5 % vanadium),

1.1.9Grade 11—UNS R52250. Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.10Grade 12—UNS R53400. Titanium alloy (0.3 % molybdenum, 0.8 % nickel),

1.1.11Grade 13—UNS R53413. Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.12Grade 14—UNS R53414. Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.13Grade 15—UNS R53415. Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.14Grade 16—UNS R52402. Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.14.1Grade 16H—UNS R52402. Unalloyed titanium plus 0.04 to 0.08 % palladium (Grade 16 with 58 ksi (400 MPa) minimum UTS),

1.1.15Grade 17—UNS R52252. Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.16Grade 18—UNS R56322. Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.04 to 0.08 % palladium,

1.1.17Grade 19—UNS R58640. Titanium alloy (3 % aluminum, 8 % vanadium, 6 % chromium, 4 % zirconium, 4 % molybdenum),

1.1.18Grade 20—UNS R58645. Titanium alloy (3 % aluminum, 8 % vanadium, 6 % chromium, 4 % zirconium, 4 % molybdenum) plus 0.04 to 0.08 % palladium,

1.1.19Grade 21—UNS R58210. Titanium alloy (15 % molybdenum, 3 % aluminum, 2.7 % niobium, 0.25 % silicon),

1.1.20Grade 23—UNS R56407. Titanium alloy (6 % aluminum, 4 % vanadium with extra low interstitial elements, ELI),

1.1.21Grade 24—UNS R56405. Titanium alloy (6 % aluminum, 4 % vanadium) plus 0.04 % to 0.08 % palladium,

1.1.22Grade 25—UNS R56403. Titanium alloy (6 % aluminum, 4 % vanadium) plus 0.3 to 0.8 % nickel and 0.04 to 0.08 % palladium,

1.1.23Grade 26—UNS R52404. Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.23.1Grade 26H—UNS R52404. UNS RUnalloyed titanium plus 0.08 to 0.14 % ruthenium (Grade 26 with 58 ksi (400 MPa) minimum UTS),

1.1.24Grade 27—UNS R52254. Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.25Grade 28—UNS R56323. Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.08 to 0.14 % ruthenium,

1.1.26Grade 29—UNS R56404. Titanium alloy (6 % aluminum, 4 % vanadium with extra low interstitial elements, ELI) plus 0.08 to 0.14 % ruthenium,

1.1.27Grade 32—UNS R55111. Titanium alloy (5 % aluminum, 1 % tin, 1 % vanadium, 1 % zirconium, 0.8 % molybdenum),

1.1.28Grade 33—UNS R53442. Titanium alloy (0.4 % nickel, 0.015 % palladium, 0.025 % ruthenium, 0.15 % chromium),

1.1.29Grade 34—UNS R53445. Titanium alloy (0.4 % nickel, 0.015 % palladium, 0.025 % ruthenium, 0.15 % chromium),

1.1.30Grade 35—UNS R56340. Titanium alloy (4.5 % aluminum, 2 % molybdenum, 1.6 % vanadium, 0.5 % iron, 0.3 % silicon),

1.1.31Grade 36—UNS R58450. Titanium alloy (45 % niobium),

1.1.32Grade 37—UNS R52815. Titanium alloy (1.5 % aluminum),

1.1.33Grade 38—UNS R54250. Titanium alloy (4 % aluminum, 2.5 % vanadium, 1.5 % iron), and

1.1.34Grade 39—UNS R53390. Titanium alloy (0.25 % iron, 0.4 % silicon).

Note 1:H grade material is identical to the corresponding numeric grade (that is, Grade 2H = Grade 2) except for the higher guaranteed minimum UTS, and may always be certified as meeting the requirements of its corresponding numeric grade. Grades 2H, 7H, 16H, and 26H are intended primarily for pressure vessel use.

1.2The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

ASTM E 1447 : 2001 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity Method
ASTM E 1409 : 2013 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by Inert Gas Fusion
ASTM E 1941 : 2010 : R2016 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys by Combustion Analysis
ASTM E 2371 : 2013 Standard Test Method for Analysis of Titanium and Titanium Alloys by Direct Current Plasma and Inductively Coupled Plasma Atomic Emission Spectrometry (Performance-Based Test Methodology)
ASTM E 1941 : 2010 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys by Combustion Analysis
ASTM E 1409 : 2004 Standard Test Method for Determination of Oxygen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
ASTM E 1447 : 1992 : R1996 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity Method
ASTM E 1409 : 2005 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
ASTM E 1447 : 2004 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity Method
ASTM E 1447 : 2009 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity/Infrared Detection Method
ASTM E 2626 : 2008 Standard Guide for Spectrometric Analysis of Reactive and Refractory Metals
ASTM E 1941 : 2004 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys
ASTM E 2371 : 2004 Standard Test Method for Analysis of Titanium and Titanium Alloys by Atomic Emission Plasma Spectrometry (Withdrawn 2013)
ASTM E 1447 : 2009 : R2016 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by Inert Gas Fusion Thermal Conductivity/Infrared Detection Method
ASTM E 2626 : 2008 : EDT 1 Standard Guide for Spectrometric Analysis of Reactive and Refractory Metals (Withdrawn 2017)
ASTM E 1409 : 1997 Standard Test Method for Determination of Oxygen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
ASTM E 1409 : 2008 Standard Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
ASTM E 1941 : 1998 Standard Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys
ASTM E 1447 : 2005 Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity/Infrared Detection Method

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.