ASTM B 867 : 1995 : R2013
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Electrodeposited Coatings of Palladium-Nickel for Engineering Use
Hardcopy , PDF
09-11-2023
English
01-12-2013
CONTAINED IN VOL. 02.05, 2017 Provides requirements for electrodeposited palladium-nickel coatings containing between 70 and 95 mass % of palladium metal.
Committee |
B 08
|
DocumentType |
Standard
|
Pages |
10
|
ProductNote |
Reconfirmed 2013
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1Composition—This specification covers requirements for electrodeposited palladium-nickel coatings containing between 70 and 95 mass % of palladium metal. Composite coatings consisting of palladium-nickel and a thin gold overplate for applications involving electrical contacts are also covered.
1.2Properties—Palladium is the lightest and least noble of the platinum group metals. Palladium-nickel is a solid solution alloy of palladium and nickel. Electroplated palladium-nickel alloys have a density between 10 and 11.5, which is substantially less than electroplated gold (17.0 to 19.3) and comparable to electroplated pure palladium (10.5 to 11.8). This yields a greater volume or thickness of coating per unit mass and, consequently, some saving of metal weight. The hardness range of electrodeposited palladium-nickel compares favorably with electroplated noble metals and their alloys (1, 2).2
Approximate Hardness (HK25) | |
Gold | 50–250 |
Palladium | 75–600 |
Platinum | 150–550 |
Palladium-Nickel | 300–650 |
Rhodium | 750–1100 |
Ruthenium | 600–1300 |
1.3The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
ASTM B 818 : 2003 : R2018 | Standard Specification for Cobalt-Chromium-Nickel-Molybdenum-Tungsten Alloy<brk/>(UNS R31233) Plate, Sheet and Strip |
ASTM B 741 : 1995 : R2000 | Standard Test Method for Porosity In Gold Coatings On Metal Substrates By Paper Electrography (Withdrawn 2005) |
ASTM B 343 : 1992 : REV A : R2004 : EDT 1 | Standard Practice for Preparation of Nickel for Electroplating with Nickel |
ASTM B 845 : 1997 | Standard Guide for Mixed Flowing Gas (MFG) Tests for Electrical Contacts |
ASTM B 507 : 2014 : REDLINE | Standard Practice for Design of Articles to Be Electroplated on Racks |
ASTM B 542 : 2013 : REDLINE | Standard Terminology Relating to Electrical Contacts and Their Use |
ASTM B 849 : 2002 | Standard Specification for Pre-Treatments of Iron or Steel for Reducing Risk of Hydrogen Embrittlement |
ASTM B 765 : 2003 : R2018 | Standard Guide for Selection of Porosity and Gross Defect Tests for Electrodeposits and Related Metallic Coatings |
ASTM D 1125 : 2014 : REDLINE | Standard Test Methods for Electrical Conductivity and Resistivity of Water (Withdrawn 2023) |
ASTM B 818 : 2003 : R2018 | Standard Specification for Cobalt-Chromium-Nickel-Molybdenum-Tungsten Alloy<brk/>(UNS R31233) Plate, Sheet and Strip |
ASTM B 489 : 1985 : R2018 | Standard Practice for Bend Test for Ductility of Electrodeposited and Autocatalytically Deposited Metal Coatings on Metals |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.