ASTM B 952/B952M : 2009
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for Zinc Alloys in Ingot Form for Spin Casting
Hardcopy , PDF
11-11-2014
English
01-10-2009
Committee |
B 02
|
DocumentType |
Standard
|
Pages |
3
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This specification covers zinc alloys in ingot form for remelting for the manufacture of Spin Castings as specified and designated, as shown in Table 1. Seven alloy compositions are specified, designated as follows:
Common | Traditional | UNS |
Spin Casting Alloy SC-A | ... | ... |
Spin Casting Alloy SC-B | ... | ... |
Spin Casting Alloy SC-C | ... | ... |
Spin Casting Alloy SC-D | HJ10 | ... |
Spin Casting Alloy SC-E | HJ20 | ... |
Spin Casting Alloy SC-F | HJ40 | ... |
ZA-73 | ... | ... |
1.2 Zinc alloys #2, #3, #5, and ZA-8 specified in Specification B240 are also used in the spin casting process.
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.
TABLE 1 Chemical and North American Color Code Requirements
Alloy SC-A | Alloy SC-B | Alloy SC-C | ZA-73 | Alloy SC-D | Alloy SC-E | Alloy SC-F | |
Color CodeA | |||||||
ElementB | |||||||
Aluminum | 3.9–4.3 | 3.9–4.3 | 3.4–4.6 | 7.7–8.0 | 3.2–3.8 | 3.2-3.8 | 3.25-3.75 |
Magnesium | 0.1–0.2 | 0.4–0.6 | 0.4–0.43 | 0.02–0.03 | 0.15-0.30 | 0.45-0.75 | 0.45-4.75 |
Copper | 2.6–2.9 | 2.7–3.3 | 1.3–1.4 | 3.0–3.3 | 1.2-1.8 | 2.5-3.25 | 4.25-4.75 |
Iron, max | 0.035 | 0.035 | 0.10 | 0.075 | 0.035 | 0.075 | 0.035 |
Lead, max | 0.004 | 0.004 | 0.015 | 0.005 | 0.004 | 0.005 | 0.004 |
Cadmium, max | 0.0030 | 0.0030 | 0.005 | 0.003 | 0.003 | 0.003 | 0.003 |
Tin, max | 0.0015 | 0.0015 | 0.005 | 0.002 | 0.002 | 0.003 | 0.002 |
Nickel, max | ... | ... | 0.02 | ... | . . . | 0.02 | . . . |
Zinc | Remainder | Remainder | Remainder | Remainder | Remainder | Remainder | Remainder |
A Per Practice B908.
B For purposes of acceptance and rejection, the observed value or calculated value obtained from analysis should be rounded to the nearest unit in the last right-hand place of figures, used in expressing the specific limit in accordance with the rounding procedure prescribed in Practice E29.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.