• Shopping Cart
    There are no items in your cart

ASTM D 1795 : 1996 : R2007 : EDT 1

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Standard Test Method for Intrinsic Viscosity of Cellulose

Available format(s)

Hardcopy , PDF

Superseded date

11-11-2014

Superseded by

ASTM D 1795 : 2013

Language(s)

English

Published date

01-06-2007

€67.30
Excluding VAT

Committee
D 01
DocumentType
Test Method
Pages
6
ProductNote
Reconfirmed EDT 1
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1 This test method covers the determination of the intrinsic viscosity of purified celluloses such as bleached wood pulps, cotton linters, and regenerated cellulose. It is applicable to all cellulose samples with an intrinsic viscosity of 15 dl/g or less. Most native (unpurified) celluloses have intrinsic viscosity values too high for measurement by this test method.

Note 1 - The use of cuprammonium hydroxide solution for regular viscosity determination is described in Method T 206 m-55 of the Technical Association of Pulp and Paper Industry on "Cuprammonium Disperse Viscosity of Pulp," and Joint Army-Navy Specifications JAN-C-206.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.