• There are no items in your cart

ASTM D 2256/D2256M : 2010 : EDT 1

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Standard Test Method for Tensile Properties of Yarns by the Single-Strand Method

Available format(s)

Hardcopy , PDF

Superseded date

11-11-2014

Language(s)

English

Published date

01-06-2010

€74.48
Excluding VAT

CONTAINED IN VOL. 07.01, 2015 Defines the determination of tensile properties of monofilament, multifilament, and spun yarns, either single, plied, or cabled with the exception of yarns that stretch more than 5.0% when tension is increased from 0.05 to 1.0 cN/tex (0.5 to 1.0 gf/tex).

Committee
D 13
DevelopmentNote
Supersedes ASTM D 2256. (08/2009)
DocumentType
Test Method
Pages
13
ProductNote
Reconfirmed EDT 1
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1 This test method covers the determination of tensile properties of monofilament, multifilament, and spun yarns, either single, plied, or cabled with the exception of yarns that stretch more than 5.0 % when tension is increased from 0.05 to 1.0 cN/tex [0.5 to 1.0 gf/tex].

1.2 This test method covers the measurement of breaking force and elongation of yarns and includes directions for the calculation of breaking tenacity, initial modulus, chord modulus, and breaking toughness.

1.2.1 Options are included for the testing of specimens in: (A) straight, (B) knotted, and (C) looped form.

1.2.2 Conditions of test are included for the testing of specimens that are: (1) conditioned air, (2) wet, not immersed, (3) wet, immersed, (4) oven-dried, (5) exposed to elevated temperature, or (6) exposed to low temperature.

Note 1—Special methods for testing yarns made from specific fibers; namely, glass, flax, hemp, ramie, and kraft paper and for specific products; namely, tire cords and rope, have been published: Test Methods D885, and Specification D578.

Note 2—For directions covering the determination of breaking force of yarn by the skein method refer to Test Method D1578.

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

ASTM D 2258 : 1999 Standard Practice for Sampling Yarn for Testing
ASTM D 578 : 2005 Standard Specification for Glass Fiber Strands
ASTM D 76 : 1999 Standard Specification for Tensile Testing Machines for Textiles
ASTM D 1578 : 1993 Standard Test Method for Breaking Strength of Yarn in Skein Form

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.