ASTM D 3654/D3654M : 2000 : EDT 1
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Test Methods for Shear Adhesion of Pressure-Sensitive Tapes
English
10-04-2000
11-11-2014
| Committee |
D 10
|
| DocumentType |
Test Method
|
| Pages |
6
|
| PublisherName |
American Society for Testing and Materials
|
| Status |
Superseded
|
| SupersededBy |
1.1 This test method describes procedures for determining the ability of pressure-sensitive tapes to remain adhered under constant load applied parallel to the surface of the tape and substrate.
1.1.1 Procedure A measures the shear adhesion when applied to a vertical standard steel panel.
1.1.2 Procedure B measures the shear adhesion when applied to vertical panel covered with NIST SRM 1810A standard fiberboard.
1.1.3 Procedure C measures the shear adhesion when applied to a vertical panel covered with a fiberboard as defined by Comite Europeen de Normalisation (CEN).
1.1.4 Procedure D measures shear adhesion when applied to a vertical panel covered with a fiberboard agreed upon by the buyer and seller.
1.1.5 Procedure E measures shear adhesion of filament reinforced tape when applied to a horizontal standard steel panel.
1.1.6 Procedure F measures shear adhesion of a filament reinforced tape when applied to a horizontal panel covered with NIST SRM 1810A standard fiberboard.
1.1.7 Procedure G measures the shear adhesion of a filament reinforced tape when applied to a horizontal panel covered with a standard fiberboard defined by CEN.
1.1.8 Procedure H measures the shear adhesion the same as Procedure A except the test is conducted at an elevated temperature and after a 10-min dwell time at the elevated temperature.
1.2 These procedures provide a means of assessing the uniformity of the adhesive of a given type of pressure-sensitive tape, usually tapes used for packaging applications. The assessment may be within a roll of tape, between rolls or production lots.
1.2.1 Variations in the tape backing and adhesive affect the response; therefore, these procedures cannot be used to pinpoint the specific cause(s) of nonuniformity.
1.2.2 This test method is intended to replace AFERA 4012, CEN 1943, and PSTC (see 7.2).