10-04-1998
CONTAINED IN VOL. 08.02, 2014 Determines a degradation-end point (a brittle point) for degradable polyethylene/polypropylene films and sheeting less than 1.0 mm (0.04 in) thick.
Committee |
D 20
|
DocumentType |
Standard Practice
|
Pages |
4
|
ProductNote |
Reconfirmed 2002
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This practice covers the determination of a degradation-end point (a brittle point) for degradable polyethylene/polypropylene films and sheeting less than 1.0 mm (0.04 in.) thick. This practice is not intended for determination of the rate of degree of degradation of a polyethylene/polypropylene film or sheet, but rather, to assess when in the course of its degradation under some condition, a brittle point is reached. If one wishes to monitor tensile elongation during the degradation process (such as when the tensile elongation is significantly greater than 5 %), Test Method D 882 is recommended. This practice should not be considered the only way of determining a degradation-end point.
1.2 Tensile properties of plastics 1.0 mm (0.04 in.) or greater in thickness shall be determined in accordance with Test Method D 638.
1.3 Use a static weighing-constant rate of grip separation test. This procedure employs a constant rate of separation of the grips holding the sample and a static load cell.
Note 1—This procedure is based on the use of grip separation as a measure of extension; however, the desirability of using extension indicators accurate to ±1.0 % or better as specified in Test Method D 638 is recognized, and a provision for the use of such instrumentation is incorporated in the procedure.
1.4 This procedure has been successful for determining the degradation end point of ethylene-carbon-monoxide copolymers and has screened successfully two other additive-type polyethylenes in a round robin test.
1.5 The values stated in SI units are to be regarded as the standard. The values in parentheses are for information only.
1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
1.7 There is no equivalent ISO standard.
ASTM D 7475 : 2011 | Standard Test Method for Determining the Aerobic Degradation and Anaerobic Biodegradation of Plastic Materials under Accelerated Bioreactor Landfill Conditions |
ASTM D 5208 : 2014 | Standard Practice for Fluorescent Ultraviolet (UV) Exposure of Photodegradable Plastics |
ASTM D 5071 : 2006 : R2013 | Standard Practice for Exposure of Photodegradable Plastics in a Xenon Arc Apparatus |
ASTM D 6954 : 2018 | Standard Guide for Exposing and Testing Plastics that Degrade in the Environment by a Combination of Oxidation and Biodegradation |
ASTM D 5272 : 2008 : R2013 | Standard Practice for Outdoor Exposure Testing of Photodegradable Plastics |
ASTM D 618 : 2013 : REDLINE | Standard Practice for Conditioning Plastics for Testing |
ASTM D 5208 : 2014 : REDLINE | Standard Practice for Fluorescent Ultraviolet (UV) Exposure of Photodegradable Plastics |
ASTM D 638 : 2014 : REDLINE | Standard Test Method for Tensile Properties of Plastics |
ASTM D 374 : 1999 | Standard Test Methods for Thickness of Solid Electrical Insulation |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.