ASTM D 4414 : 1995 : R2007
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Practice for Measurement of Wet Film Thickness by Notch Gages
Hardcopy , PDF
11-11-2014
English
01-06-2007
CONTAINED IN VOL. 06.01, 2018 Outlines the use of thin rigid metal notched gages, also called step or comb gages, in the measurement of wet film thickness of organic coatings, such as paint, varnish and lacquer.
Committee |
D 01
|
DocumentType |
Standard Practice
|
Pages |
3
|
ProductNote |
Reconfirmed 2007
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1 This practice describes the use of thin rigid metal notched gages, also called step or comb gages, in the measurement of wet film thickness of organic coatings, such as paint, varnish, and lacquer.
1.2 Notched gage measurements are neither accurate nor sensitive, but they are useful in determining approximate wet film thickness of coatings on articles where size(s) and shape(s) prohibit the use of the more precise methods given in Test Methods D 1212.
1.3 This practice is divided into the following two procedures:
1.3.1 Procedure A - A square or rectangular rigid metal gage with notched sides is used to measure wet film thicknesses ranging from 3 to 2000 m (0.5 to 80 mils 1). Such a gage is applicable to coatings on flat substrates and to coatings on articles of various sizes and complex shapes where it is possible to get the end tabs of the gage to rest in the same plane on the substrate.
1.3.2 Procedure B - A circular thin rigid metal notched gage is used to measure wet film thicknesses ranging from 25 to 2500 m (1 to 100 mils ). Such a gage is applicable to coatings on flat substrates and to coatings on objects of various sizes and complex shapes.
1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
ASTM E 1795 : 2017 | Standard Specification for Non-Reinforced Liquid Coating Encapsulation Products for Leaded Paint in Buildings |
ASTM D 823 : 2018 | Standard Practices for Producing Films of Uniform Thickness of Paint, Coatings and Related Products on Test Panels |
ASTM D 3276 : 2015 : EDT 1 | Standard Guide for Painting Inspectors (Metal Substrates) |
ASTM D 7394 : 2018 | Standard Practice for Rheological Characterization of Architectural Coatings using Three Rotational Bench Viscometers |
ASTM D 6237 : 2009 : R2015 | Standard Guide for Painting Inspectors (Concrete and Masonry Substrates) |
ASTM E 1797 : 2012 : R2017 : EDT 1 | Standard Specification for Reinforced Liquid Coating Encapsulation Products for Leaded Paint in Buildings |
ASTM D 711 : 2010 : R2015 | Standard Test Method for No-Pick-Up Time of Traffic Paint |
ASTM D 5498 : 2012 : REV A : R2018 | Standard Guide for Developing a Training Program for Personnel Performing Coating and Lining Work Inspection for Nuclear Facilities |
ASTM D 7377 : 2009 : R2018 | Standard Practice for Evaluating the Water Wash-Off Resistance of Traffic Paints using a Water Faucet |
ASTM D 1212 : 1991 | Standard Test Methods for Measurement of Wet Film Thickness of Organic Coatings |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.