• There are no items in your cart

ASTM D 6007 : 2002

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Standard Test Method for Determining Formaldehyde Concentration in Air from Wood Products Using a Small Scale Chamber

Available format(s)

Hardcopy , PDF

Superseded date

11-11-2014

Language(s)

English

Published date

10-04-2002

€67.30
Excluding VAT

Committee
D 07
DocumentType
Test Method
Pages
9
ProductNote
Reconfirmed 2002
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1 This test method measures the formaldehyde concentrations in air from wood products under defined test conditions of temperature and relative humidity. Results obtained from this small-scale chamber test method are intended to be comparable to results obtained testing larger product samples by the large chamber test method for wood products, Test Method E 1333. The results may be correlated to values obtained from Test Method E 1333. The quantity of formaldehyde in an air sample from the small chamber is determined by a modification of the National Institute for Occupational Safety and Health (NIOSH) 3500 chromotropic acid test procedure. Other analytical procedures may be used to determine the quantity of formaldehyde in the air sample provided that such methods give results comparable to those obtained by using the chromotropic acid procedure. However, the test results and test report must be properly qualified and the analytical procedure employed must be accurately described.

1.2 The wood-based panel products to be tested by this test method are characteristically used for different applications and are tested at different relative amounts or loading ratios to reflect different applications. This is a test method that specifies testing at various loading ratios for different product types. However, the test results and test report must be properly qualified and must specify the make-up air flow, sample surface area, and chamber volume.

1.3 Ideal candidates for small-scale chamber testing are products relatively homogeneous in their formaldehyde release characteristics. Still, product inhomogeneities must be considered when selecting and preparing samples for small-scale chamber testing.

1.4 The values stated in SI units are the standard values. Any values given in parentheses are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

ASTM D 5116 : 2017 Standard Guide for Small-Scale Environmental Chamber Determinations of Organic Emissions from Indoor Materials/Products
ASTM D 8141 : 2017 Standard Guide for Selecting Volatile Organic Compounds (VOCs) and Semi-Volatile Organic Compounds (SVOCs) Emission Testing Methods to Determine Emission Parameters for Modeling of Indoor Environments
ASTM D 6330 : 1998 : R2014 Standard Practice for Determination of Volatile Organic Compounds (Excluding Formaldehyde) Emissions from Wood-Based Panels Using Small Environmental Chambers Under Defined Test Conditions
ASTM D 7911 : 2014 Standard Guide for Using Reference Material to Characterize Measurement Bias Associated with Volatile Organic Compound Emission Chamber Test
ASTM D 7706 : 2017 Standard Practice for Rapid Screening of VOC Emissions from Products Using Micro-Scale Chambers

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.