Standard Methods for Chemical Analysis of Ferrocolumbium
Hardcopy , PDF
11-11-2014
English
10-10-2002
Committee |
E 01
|
DocumentType |
Test Method
|
Pages |
6
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy |
1.1 These methods cover the chemical analysis of ferrocolumbium having chemical compositions within the following limits:
Element | Concentration, % |
Aluminum | 2.00 max |
Carbon | 0.30 max |
Chromium | 2.00 max |
Cobalt | 0.25 max |
Niobium | 40.00 to 75.00 |
Lead | 0.01 max |
Manganese | 3.00 max |
Phosphorus | 0.05 max |
Silicon | 4.00 max |
Sulfur | 0.03 max |
Tantalum | 7.00 max |
Tin | 0.15 max |
Titanium | 5.00 max |
Tungsten | 0.50 max |
1.2 The methods appear in the following order:
Sections | |
Niobium, Tantalum, and Titanium by the | |
Ion-Exchange Method | 9-30 |
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 5.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.