BIS IS 13655 : 1993(R2000)
Current
The latest, up-to-date edition.
GUIDELINES FOR HEAT TREATMENT OF CAST IRON
12-01-2013
FOREWORD
1 SCOPE
2 HEAT-TREATMENT OF GREY CAST IRON
3 HEAT-TREATMENT OF DUCTILE IRON
4 HEAT-TREATMENT OF MALLEABLE CAST IRON
5 HEAT-TREATMENT OF AUSTENITIC CAST IRON
6 FURNACES
7 PRECAUTIONS
8 MICRO-STRUCTURE AND HARDNESS
Specifies the method of heat treatment for the following types of cast iron. a.) Cast iron (other than Austenitic) - Unalloyed and alloyed: - Grey iron, - Ductile iron, and - Malleable iron. b.) Austenitic cast iron: - Flake graphite (AFG), and - Spheroidal graphite (ASG).
Committee |
MTD 22
|
DocumentType |
Standard
|
PublisherName |
Bureau of Indian Standards
|
Status |
Current
|
BIS IS 210 : 2009(R2014) | GREY IRON CASTINGS - SPECIFICATION |
BIS IS 2108 : 1977 | BLACKHEART MALLEABLE IRON CASTINGS |
BIS IS 3355 : 1974(R2005) | GREY IRON CASTINGS FOR ELEVATED TEMPERATURES FOR NON-PRESSURE CONTAINING PARTS |
BIS IS 5787 : 1986(R2000) | SPHEROIDAL OR NODULAR GRAPHITE IRON CASTINGS FOR PAPER MILL DRYER ROLLS |
BIS IS 2749 : 1974(R2005) | AUSTENITIC IRON CASTINGS |
BIS IS 5789 : 1993(R1999) | AUSTENITIC SPHEROIDAL GRAPHITE IRON CASTINGS FOR PRESSURE CONTAINING PARTS SUITABLE FOR LOW-TEMPERATURE SERVICE - SPECIFICATION |
BIS IS 7520 : 1974(R2005) | CORROSION RESISTANT HIGH SILICON IRON CASTINGS |
BIS IS 1865 : 1991(R2005) | IRON CASTINGS WITH SPHEROIDAL OR NODULAR GRAPHITE - SPECIFICATION |
BIS IS 2640 : 1977 | PEARLITIC MALLEABLE IRON CASTINGS |
BIS IS 4771 : 1985(R2005) | ABRASION-RESISTANT IRON CASTINGS |
BIS IS 6331 : 1987(R2005) | AUTOMOTIVE GREY IRON CASTINGS |
BIS IS 210 : 2009(R2014) | GREY IRON CASTINGS - SPECIFICATION |
BIS IS 2107 : 1977 | WHITEHEART MALLEABLE IRON CASTINGS |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.