BS 2TA 41:2009
Current
The latest, up-to-date edition.
Specification for forging stock of titanium- aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1205-1375 MPa) (limiting ruling section over 25 mm up to and including 75 mm)
Hardcopy , PDF
English
30-11-2009
Foreword
1 Scope
2 Normative references
3 Technical requirements
Bibliography
Describes requirements for titanium-aluminium-molybdenum-tin-silicon-carbon alloy forging stock with a tensile strength of 1205 MPa to 1375 MPa.
| Committee |
ACE/61/-/49
|
| DevelopmentNote |
Supersedes BS TA41(1971) and 09/30193175 DC. (11/2009)
|
| DocumentType |
Standard
|
| Pages |
10
|
| PublisherName |
British Standards Institution
|
| Status |
Current
|
| Supersedes |
This British Standard specifies requirements for titanium-aluminium-molybdenum-tin-silicon-carbon alloy forging stock with a tensile strength of 1 205 MPa to 1 375 MPa.
| PREN 4500-004 : 200P2 | AEROSPACE SERIES - METALLIC MATERIALS - RULES FOR DRAFTING AND PRESENTATION OF MATERIAL STANDARDS - PART 004: SPECIFIC RULES FOR TITANIUM AND TITANIUM ALLOYS |
| PREN 4500-001 : 200P2 | AEROSPACE SERIES - METALLIC MATERIALS - RULES FOR DRAFTING AND PRESENTATION OF MATERIAL STANDARDS - PART 001: GENERAL RULES |
| BS 2TA 100:1973 | Procedure for inspection and testing of wrought titanium and titanium alloys |
| BS TA 38:1971 | Specification for bar for machining of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1250-1420 N/mm<sup>2</sup>) (limiting ruling section 25 mm) |
| BS TA 42:1971 | Specification for forgings of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1205-1375 N/mm<sup>2</sup>) (limiting ruling section over 25 mm up to and including 75 mm) |
| BS TA 40:1971 | Specification for bar for machining of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1205-1375 N/mm<sup>2</sup>) (limiting ruling section over 25 mm up to and including 75 mm) |
| BS TA 39:1971 | Specification for forging stock of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1250-1420 N/mm<sup>2</sup>) (limiting ruling section 25 mm) |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.