• Shopping Cart
    There are no items in your cart

DEFSTAN 03-31/1(1993) : 1993

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

A GUIDE TO THE USE OF CHROMIUM PLATING FOR ENGINEERING PURPOSES

Available format(s)

Hardcopy , PDF

Superseded date

03-03-2008

Language(s)

English

Published date

01-01-1993

€14.02
Excluding VAT

Preface
Section One - General
0 Introduction
1 Scope
2 WARNING
3 Related Documents
4 Types of Chromium Coatings
Section Two - Requirements
5 Suitability for Chromium Plating
6 Type-Testing of Chromium Plated Items
7 Selection of Basis Materials
8 Reclamation of Worn or Over-Machined Items
9 Avoidance of Stress Concentrations
10 Mechanical Pre-Treatment of Items
11 Dimensional Tolerances
12 Thickness Requirements
13 Properties of Chromium Plated Parts
14 Machining and Grinding
15 Defective Plating
16 Plating with Other Metals on Areas not Chromium Plated

Gives guidance for the use of chromium plating for engineering purposes.

DevelopmentNote
Supersedes DG-13 (07/2003)
DocumentType
Standard
Pages
14
PublisherName
UK Ministry of Defence Standards
Status
Superseded
SupersededBy

DEFSTAN 02-870/2(2004) : 2004 CHROMIUM PLATING FOR THE RECLAMATION OF ENGINEERING COMPONENTS
DEFSTAN 03-4/5(2006) : 2006 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 07-85(PT1)/3(2006) : 2006 DESIGN REQUIREMENTS FOR WEAPONS AND ASSOCIATED SYSTEMS - PART 1: MANDATORY DESIGN REQUIREMENTS
DEFSTAN 03-4/4(1998) : 1998 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-4/6(2011) : 2011 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-14/3(2005) : 2005 ELECTRO-DEPOSITION OF CHROMIUM FOR ENGINEERING PURPOSES
SAE AMS03_4A The Pre-Treatment and Protection of Steel Items of Specified Maximum Tensile Strength Exceeding 1450 MPa
DEFSTAN 03-14/2(1995) : 1995 ELECTRO-DEPOSITION OF CHROMIUM FOR ENGINEERING PURPOSES
DEFSTAN 03-38/1(2007) : 2007 GUIDANCE FOR THE USE OF ALTERNATIVES TO HEXAVALENT CHROMIUM FOR THE PROTECTIVE COATING OF DEFENCE EQUIPMENT

DEFSTAN 03-4/4(1998) : 1998 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-21/3(2002) : 2002 MECHANICAL METHODS FOR THE INDUCEMENT OF RESIDUAL SURFACE COMPRESSIVE STRESSES
BS 4479:1969 Recommendations for the design of metal articles that are to be coated
DEFSTAN 03-27/2(1998) : 1998 ELECTRODEPOSITION OF NICKEL FOR ENGINEERING PURPOSES
DEFSTAN 03-14/2(1995) : 1995 ELECTRO-DEPOSITION OF CHROMIUM FOR ENGINEERING PURPOSES

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.