WROUGHT COPPER ALLOYS - COPPER-ALUMINIUM ALLOYS - (ALUMINIUM BRONZE) - COMPOSITION
01-10-2000
12-01-2013
Kein Inhaltsverzeichnis in der Norm vorhanden.
Specifies the composition of wrought copper alloy semi-finished products containing aluminium as the main alloying element. Table 1 provides information on typical properties and preferred use of particular copper-aluminium alloys. The examples given do not claim to be generally valid or complete.
DocumentType |
Standard
|
PublisherName |
German Institute for Standardisation (Deutsches Institut für Normung)
|
Status |
Withdrawn
|
Standards | Relationship |
ISO 428:1983 | Similar to |
DIN ISO 5182:1995-03 | WELDING - MATERIALS FOR RESISTANCE WELDING ELECTRODES AND ANCILLARY EQUIPMENT |
DIN 8566-2:1984-12 | FILLER METALS FOR THERMAL SPRAYING; SOLID WIRES FOR ARC SPRAYING; TECHNICAL DELIVERY CONDITIONS |
DIN 1785:1983-10 | WROUGHT COPPER AND COPPER ALLOY TUBES FOR CONDENSERS AND HEAT EXCHANGERS |
DIN 1733-1:1988-06 | WELDING FILLER METALS FOR COPPER AND COPPER ALLOYS - COMPOSITION, APPLICATION AND TECHNICAL DELIVERY CONDITIONS |
DIN V 17900:1999-03 | COPPER AND COPPER ALLOYS - EUROPEAN MATERIALS - COMPENDIUM OF COMPOSITIONS AND PRODUCTS |
DIN 17670-1:1983-12 | WROUGHT COPPER AND COPPER ALLOY PLATE, SHEET AND STRIP - PROPERTIES |
DIN 17660:1983-12 | WROUGHT COPPER ALLOYS - COPPER-ZINC ALLOYS - (BRASS) - (SPECIAL BRASS) - COMPOSITION |
ISO 4743:1984 | Copper alloys Determination of nickel content Titrimetric method |
DIN 17679:1983-10 | TUBES OF COPPER AND WROUGHT COPPER ALLOYS WITH ROLLED FINS FOR HEAT EXCHANGERS |
DIN 17660:1983-12 | WROUGHT COPPER ALLOYS - COPPER-ZINC ALLOYS - (BRASS) - (SPECIAL BRASS) - COMPOSITION |
DIN 50503:1998-05 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS - DETERMINATION OF COPPER IN WROUGHT AND CAST COPPER ALLOYS |
DIN 50510:1980-04 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS; DETERMINATION OF ARSENIC IN COPPER AND COPPER ALLOYS, PHOTOMETRIC METHOD |
ISO 4751:1984 | Copper and copper alloys Determination of tin content Spectrometric method |
DIN 50509:1977-05 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS, DETERMINATION OF THE ALUMINIUM CONTENT OF COPPER ALLOYS, VOLUMETRIC METHOD |
DIN 1780:1974-06 | STRIP AND STRIP CUT TO LENGTH FOR LEAF SPRINGS OF WROUGHT COPPER ALLOYS - TECHNICAL CONDITIONS OF DELIVERY |
DIN 17670-1:1983-12 | WROUGHT COPPER AND COPPER ALLOY PLATE, SHEET AND STRIP - PROPERTIES |
DIN 50504:1973-10 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS; PHOTOMETRIC DETERMINATION OF IRON IN COPPER AND COPPER ALLOYS CONTAINING 0,4% OF IRON AT MAXIMUM |
ISO 4748:1984 | Copper alloys — Determination of iron content — Na2EDTA titrimetric method |
DIN 17663:1983-12 | WROUGHT COPPER ALLOYS - COPPER-NICKEL-ZINC ALLOYS - (NICKEL SILVER) - COMPOSITION |
DIN 17662:1983-12 | WROUGHT COPPER ALLOYS - COPPER-TIN ALLOYS - (TIN BRONZE) - COMPOSITION |
DIN 50507:1977-07 | Chemical analysis of copper and copper alloys; determination of lead, extracting-titration method |
ISO 4740:1985 | Copper and copper alloys Determination of zinc content Flame atomic absorption spectrometric method |
DIN 1333-2 : 1972 | PRESENTATION OF NUMERICAL DATA - ROUNDING |
DIN 17666:1983-12 | LOW ALLOY WROUGHT COPPER ALLOYS - COMPOSITION |
DIN 17664:1983-12 | WROUGHT COPPER ALLOYS - COPPER-NICKEL ALLOYS - COMPOSITION |
DIN 17670-2:1969-06 | PLATE, SHEET AND STRIP OF COPPER AND WROUGHT COPPER ALLOYS - TECHNICAL CONDITIONS OF DELIVERY |
DIN 50506:1973-10 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS; PHOTOMETRIC DETERMINATION OF NICKEL IN COPPER ALLOYS CONTAINING 2,5% OF NICKEL AT MAXIMUM |
DIN 50508:1977-06 | CHEMICAL ANALYSIS OF COPPER AND COPPER ALLOYS; DETERMINATION OF TIN AS ALLOYING ELEMENT, VOLUMETRIC METHOD |
DIN 50505:1973-10 | CHEMICAL ANALYSIS FOR COPPER AND COPPER ALLOYS; PHOTOMETRIC DETERMINATION OF MANGANESE IN COPPER ALLOYS CONTAINING 6% OF MANGANESE AT MAXIMUM |
DIN 17682:1979-08 | ROUND SPRING WIRES MADE OF WROUGHT COPPER ALLOYS - STRENGTH PROPERTIES - TECHNICAL CONDITIONS OF DELIVERY |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.