• Shopping Cart
    There are no items in your cart

EN 13674-4:2006+A1:2009

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Railway applications - Track - Rail - Part 4: Vignole railway rails from 27 kg/m to, but excluding 46 kg/m

Published date

11-11-2009

Superseded date

11-04-2019

Superseded by

EN 13674-4:2019

Sorry this product is not available in your region.
Summarise this standard

Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Information to be supplied by the purchaser
5 Steel grades
6 Dimensions, static properties, linear mass
  and tolerances
7 Manufacture
8 Qualification of the manufacturer
9 Acceptance tests
Annex A (normative) - Rail profiles
Annex B (informative) - Comparison of steel designations
                        referred to in this European Standard
                        compared to those in EN 10027-1 and
                        EN 10027-2
Bibliography

This document specifies flat bottom Vignole railway rails from 27 kg/m to, but excluding 46 kg/m.Eight pearlitic steel grades are specified covering a rail hardness range of 200 HBW to 440 HBW and include non-heat-treated non-alloy steels, non-heat-treated alloy steels, heat-treated non-alloy steels and heat-treated alloy steels.There are 15 rail profiles specified in this document, but these may not be available in all steel grades.

Committee
CEN/TC 256
DevelopmentNote
2006 Edition Re-Issued in November 2009 and incorporates AMD 1 2009. (12/2009)