Superconductivity - Part 24: Critical current measurement - Retained critical current after double bending at room temperature of Ag-sheathed Bi-2223 superconducting wires
24-08-2018
IEC 61788-24:2018 describes a test method for determining the retained critical current after double bending at room temperature of short and straight Ag- and/or Ag alloy-sheathed Bi-2223 superconducting wires that have the shape of a flat or square tape containing mono- or multicores of oxides. The wires can be laminated with copper alloy, stainless steel or Ni alloy tapes.The test method is intended for use with superconductors that have a critical current less than 300 A and an n-value larger than 5.
Committee |
CLC/SR 90
|
DocumentType |
Standard
|
PublisherName |
European Committee for Standards - Electrical
|
Status |
Current
|
Standards | Relationship |
IEC 61788-24:2018 | Identical |
NF EN IEC 61788-24 :2018 | Identical |
BS EN IEC 61788-24:2018 | Identical |
OVE EN IEC 61788-24: 2019 08 01 | Identical |
PN-EN IEC 61788-24:2019 | Identical |
SS-EN IEC 61788-24:2019 | Identical |
NEN EN IEC 61788-24 : 2018en | Identical |
I.S. EN IEC 61788-24:2018 | Identical |
SN EN IEC 61788-24:2018 | Identical |
DIN EN IEC 61788-24:2019-07 | Identical |
UNE-EN IEC 61788-24:2018 | Identical |
VDE 0390-24:2019-07 | Identical |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.