JIS K 5600-8-2:2008
Current
The latest, up-to-date edition.
Testing methods for paints -- Part 8: Evaluation of degradation of paint coatings -- Section 2: Designation of degree of blistering Part 8: Evaluation of degradation of paint coatings - Section 2: Designation of degree of blistering
English
20-02-2008
This Standard specifies a method for assessing the degree of blistering of coatings by comparison with pictorial standards.
| DocumentType |
Standard
|
| Pages |
12
|
| PublisherName |
Japanese Standards Association
|
| Status |
Current
|
| Supersedes |
| Standards | Relationship |
| ISO 4628-2:2003 | Identical |
Reaffirmed 2017
| JIS K 5600-8-1:1999 | Testing methods for paints -- Part 8: Evaluation of degradation of paint coatings -- Section 1: General principles and rating schemes Part 8: Evaluation of degradation of paint coatings - Section 1: General principles and rating schemes |
| JIS K 5552:2023 | Zinc rich primer |
| JIS K 5600-7-9:2006 | Testing methods for paints -- Part 7: Determination of resistance to cyclic corrosion conditions -- Section 9: Salt fog/dry/humidity |
| JIS K 5553:2002 | High build type Zinc rich paint |
| JIS K 5600-7-7:2008 | Testing methods for paints -- Part 7: Long-period performance of film -- Section 7: Accelerated weathering and exposure to artificial radiation (Exposure to filtered xenon-arc radiation) |
| JIS G 3318:2008 | Prepainted hot-dip zinc -- 5 % aluminium alloy-coated steel sheet and strip |
| JIS K 5981:2006 | Thermoplastic and thermosetting powder coated films |
| JIS K 5660:2003 | Synthetic resin emulsion paints, glossy type |
| JIS K 5516:2003 | Ready mixed paints (Synthetic resin type) |
| JIS K 5657:2002 | Polyurethane resin paint for steel structures |
| JIS K 5500:2000 | Glossary of terms for coating materials |
| JIS K 5629:2002 | Calcium plumbate anticorrosive paint |
| JIS K 5600-6-1:1999 | Testing methods for paints -- Part 6: Chemical property of film -- Section 1: Resistance to liquids (General methods) Part 6: Chemical property of film - Section 1: Resistance to liquids (General methods) |
| JIS G 3312:2008 | Prepainted hot-dip zinc-coated steel sheet and strip |
| JIS K 5600-7-3:1999 | Testing methods for paints -- Part 7: Long-period performance of film -- Section 3: Resistance to humidity (Intermittent condensation) Part 7: Long-period performance of film - Section 3: Resistance to humidity (Intermittent condensation) |
| JIS K 5962:2003 | Household paint for wood and metal |
| JIS K 5600-6-2:1999 | Testing methods for paints -- Part 6: Chemical property of film -- Section 2: Resistance to liquids (Water immersion method) Part 6: Chemical property - Section 2: Resistance to liquids (Water immersion method) |
| JIS G 3322:2008 | Prepainted hot-dip 55 % aluminium -- Zinc alloy-coated steel sheet and strip |
| JIS K 5659:2008 | Long durable paints for steel structures |
| JIS K 5600-7-6:2002 | Testing methods for paints -- Part 7: Long-period performance of film -- Section 6: Natural weathering |
| JIS K 5600-7-8:1999 | Testing methods for paints -- Part 7: Long-period performance of film -- Section 8: Accelerated weathering (Exposure to fluorescent UV lamps) Part 7: Long-period performance of film - Section 8: Accelated weathering (Exposure to fluorescent UV lamps) |
| JIS K 5552:2002 | Zinc rich primer |
| JIS K 5633:2002 | Etching primer |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.