NEN EN 10002-1 : 2001
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
METALLIC MATERIALS - TENSILE TESTING - PART 1: METHOD OF TEST AT AMBIENT TEMPERATURE
08-09-2009
12-01-2013
Cooperating organizations
National foreword
Brief history
Foreword
1 Object and field of application
2 References
3 Principle
4 Definitions
4.1 Gauge length (L)
4.2 Parallel length (Lc)
4.3 Elongation
4.4 Percentage elongation
4.5 Extensometer gauge length (Le)
4.6 Extension
4.7 Percentage reduction of area (Z)
4.8 Maximum force (Fm)
4.9 Stress
5 Symbols and designations
6 Test pieces
6.1 Shape and dimensions
6.2 Types
6.3 Preparation of test pieces
7 Determination of original cross-sectional area
(So)
8 Marking the original gauge length (Lo)
9 Accuracy of testing apparatus
10 Conditions of testing
10.1 Rate of the machine
10.2 Method of gripping
11 Determination of percentage elongation after
fracture (A)
12 Determination of proof strength (non-proportional
extension) (Rp)
13 Determination of proof strength (total extension)
(Rt)
14 Method of verification of permanent set strength
(Rr)
15 Test report
Annex A Types of test piece to be used for thin
products: steets, strips and flats between 0,1
mm and 3 mm thick
Annex B Types of test piece to be used in the case of
wire, bars and sections with a diameter or
thickness of less than 4 mm
Annex C Types of test piece to be used in the case of
sheets and flats of thickness equal to or
greater than 3 mm, and wire, bars and sections
of diameter or thickness equal to or greater
than 4 mm
Annex D Types of test piece to be used in the case of
tubes
Annex E Measurement of percentage elongation after
fracture, based on sub-division of the original
gauge length
Annex F List of national standards corresponding to
reference Euronorm 18
National appendix A
National appendix B
Describes the method for tensile testing of metallic materials and defines the mechanical properties which can be determined thereby at ambient temperature. Cover references, principle, definitions, symbols and designations, test pieces, determination of original cross sectional area, marking the original gauge length, accuracy of testing apparatus, conditions of testing, determination of percentage elongation after fracture, determination of proof strength, method of verification of permanent set strength, and test report.
DocumentType |
Standard
|
PublisherName |
Netherlands Standards
|
Status |
Superseded
|
Standards | Relationship |
I.S. EN 10002-1:2001 | Identical |
ISO 6892:1998 | Identical |
UNE-EN 10002-1:2002 | Identical |
DIN EN 10002-1:2001-12 | Identical |
UNI EN 10002-1 : 2004 | Identical |
BS EN 10002-1:2001 | Identical |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.