NEN EN 658-4 : 2003
Current
The latest, up-to-date edition.
ADVANCED TECHNICAL CERAMICS - MECHANICAL PROPERTIES OF CERAMIC COMPOSITES AT ROOM TEMPERATURE - PART 4: DETERMINATION OF INTERLAMINAR SHEAR STRENGTH BY COMPRESSION LOADING OF NOTCHED TEST SPECIMENS
12-01-2013
Foreword
1 Scope
2 Normative references
3 Principle
4 Terms, definitions and symbols
5 Apparatus
5.1 Test machine
5.2 Load train
5.3 Dimensions measuring devices
6 Test specimen
7 Test specimen preparation
7.1 Machining
7.2 Number of test specimens
8 Procedure
8.1 Displacement rate
8.2 Measurement of test specimens
8.3 Testing technique
8.4 Test validity
9 Calculation
9.1 Test specimen origin
9.2 Interlaminar shear strength
10 Test report
Annex A (informative) Examples of rupture
A.1 Valid rupture
A.2 Non-valid rupture
Bibliography
Describes the conditions for determination of the interlaminar shear strength of ceramic matrix composite materials with continuous fibre reinforcement at room temperature, by loading a notched test specimen in compression.
DevelopmentNote |
Supersedes NEN NVN ENV 658-4. (04/2003)
|
DocumentType |
Standard
|
PublisherName |
Netherlands Standards
|
Status |
Current
|
Supersedes |
Standards | Relationship |
UNI EN 658-4 : 2003 | Identical |
BS EN 658-4:2003 | Identical |
I.S. EN 658-4:2003 | Identical |
EN 658-4:2003 | Identical |
DIN EN 658-4:2003-05 | Identical |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.