SAE AMS1428L
Current
The latest, up-to-date edition.
Fluid, Aircraft Deicing/Anti-Icing, Non-Newtonian (Pseudoplastic), SAE Types II, III, and IV
Hardcopy , PDF
English
14-02-2023
This foundation specification (AMS1428L) and its associated category specifications (AMS1428/1 and AMS1428/2) cover three types of deicing/anti-icing fluids, each in the form of a non-Newtonian fluid.
DocumentType |
Standard
|
Pages |
27
|
PublisherName |
SAE International
|
Status |
Current
|
Supersedes |
This foundation specification (AMS1428L) and its associated category specifications (AMS1428/1 and AMS1428/2) cover three types of deicing/anti-icing fluids, each in the form of a non-Newtonian fluid.
SAE ARP4737J | Aircraft Deicing/Anti-Icing Methods |
SAE AMS2475H | Protective Treatments Magnesium Alloys |
SAE AMS5045K | Steel, Sheet and Strip 0.25 Carbon, Maximum Hard Temper |
SAE AMS4916M | Titanium Alloy Sheet, Strip, and Plate 8Al - 1Mo - 1V Duplex Annealed |
SAE AMS4376H | Plate, Magnesium Alloy 3.0Al - 1.0Zn - 0.20Mn (AZ31B-H26) Cold Rolled and Partially Annealed |
SAE AIR9968B | Viscosity Test of Thickened Aircraft Deicing/Anti-icing Fluids |
SAE AMS4037R | Aluminum Alloy, Sheet and Plate 4.4Cu - 1.5Mg - 0.60Mn (2024; -T3 Flat Sheet, -T351 Plate) Solution Heat Treated |
SAE ARP1917A | Clarification of Terms Used in Aerospace Metals Specifications |
SAE ARP 571 : 1994 | FLIGHT DECK CONTROLS AND DISPLAYS FOR COMMUNICATION AND NAVIGATION EQUIPMENT FOR TRANSPORT AIRCRAFT |
SAE AMS4911R | Titanium Alloy, Sheet, Strip, and Plate 6Al - 4V Annealed |
SAE AMSP83310A | Plastic Sheet, Polycarbonate, Transparent |
SAE ARP5485B | Endurance Time Test Procedures for SAE Type II/III/IV Aircraft Deicing/Anti-Icing Fluids |
SAE AMS2470P | Anodic Treatment of Aluminum Alloys Chromic Acid Process |
SAE AMS4049N | Aluminum Alloy, Sheet and Plate, Alclad 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (Alclad 7075; -T6 Sheet - T651 Plate) Solution and Precipitation Heat Treated |
SAE AS5900E | Standard Test Method for Aerodynamic Acceptance of AMS1424 and AMS1428 Aircraft Deicing/Anti-Icing Fluids |
SAE AMS5886D | Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 50Ni - 20Cr - 20Co - 5.8Mo - 2.2Ti - 0.45Al Consumable Electrode or Vacuum Induction Melted 2100 °F (1149 °C) Solution Heat Treated |
SAE AMS4041T | Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (2024, -T3 Sheet/-T351 Plate with 1-1/2% Alclad) Solution Heat Treated, Cold Worked and Naturally Aged |
SAE AMS2825B | Material Safety Data Sheets |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.