SAE AMS2453
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Low Stress Grinding of Steel Parts Heat Treated to 180 ksi or Over, and Low Stress Grinding of Chrome Plating Applied to Steel Parts Heat Treated to 180 ksi or Over
Hardcopy , PDF
10-09-2022
English
21-09-2020
The purpose of this specification is to establish requirements of a grinding method and to provide grinding parameters that will eliminate or minimize overheating, cracking, high residual tensile stresses, and/or other metallurgical changes that decrease structural integrity of steel parts or chrome plated steel parts (See8.2).
DocumentType |
Standard
|
Pages |
13
|
PublisherName |
SAE International
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
The purpose of this specification is to establish requirements of a grinding method and to provide grinding parameters that will eliminate or minimize overheating, cracking, high residual tensile stresses, and/or other metallurgical changes that decrease structural integrity of steel parts or chrome plated steel parts (See 8.2). This standard establishes requirements for low stress grinding of martensitic high strength steel heat-treated to 180 ksi (1241 MPa) minimum ultimate tensile strength (UTS) and above, and requirements for low stress grinding of chromium plating applied to such high strength steel.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.