SAE AMS2477A
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Conversion Coating for Aluminum Alloys Low Electrical Resistance Coating
Hardcopy , PDF
English
19-04-2010
03-09-2018
1 SCOPE
2 APPLICABLE DOCUMENTS
3 TECHNICAL REQUIREMENTS
4 QUALITY ASSURANCE PROVISIONS
5 PREPARATION FOR DELIVERY
6 ACKNOWLEDGMENT
7 REJECTIONS
8 NOTES
Specifies the requirements for a low-electrical-resistance chemical conversion coating on aluminum and aluminum alloy parts.
| DocumentType |
Standard
|
| Pages |
6
|
| PublisherName |
SAE International
|
| Status |
Superseded
|
| SupersededBy | |
| Supersedes |
This specification covers the requirements for a low-electrical-resistance chemical conversion coating on aluminum and aluminum alloy parts.
| SAE AS6116A | Aluminum Fittings, Axially Swaged Tube with Flareless Separable, Fluid System Up to 1500 psi (10340 kPa) Maximum, Specification for |
| NASA MSFC HDBK 3697 : 2014 | ELECTRICAL BONDING DESIGN GUIDE HANDBOOK |
| SAE AMS2473H | Chemical Film Treatment for Aluminum Alloys General Purpose Coating |
| MIL P 53022 : B | PRIMER, EPOXY COATING, CORROSION INHIBITING, LEAD & CHROMATE FREE |
| SAE AMS4027N | Aluminum Alloy, Sheet and Plate 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061; -T6 Sheet, -T651 Plate) Solution and Precipitation Heat Treated |
| MIL-PRF-23377 Revision K:2012 | Primer Coatings: Epoxy, High-Solids |
| MIL P 53030 : A | PRIMER COATING, EPOXY, WATER REDUCIBLE, LEAD & CHROMATE FREE |
| MIL-PRF-85582 Revision E:2012 | PRIMER COATINGS: EPOXY, WATERBORNE |
| ASTM D 3359 : 2017 : REDLINE | Standard Test Methods for Rating Adhesion by Tape Test |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.