1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Specifies a procedure for revealing the macrostructure and microstructure of titanium alloys.
| DocumentType |
Standard
|
| Pages |
5
|
| PublisherName |
SAE International
|
| Status |
Superseded
|
| SupersededBy | |
| Supersedes |
This specification covers a procedure for revealing the macrostructure and microstructure of titanium alloys.
| SAE AMS6935B | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al – 6.0V – 2.0Sn Solution Heat Treated and Aged |
| SAE AMST81556A | Titanium and Titanium Alloys, Extruded Bars and Shapes, Aircraft Quality |
| SAE AMS6932B | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al – 4.0V Extra Low Interstitial Annealed |
| SAE AMS6926B | Titanium Alloy Bars, Forgings and Forging Stock 13V - 11Cr - 3Al Solution Heat Treated and Aged |
| SAE AMS6905B | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al - 2.0Sn - 4.0Zr - 2.0Mo Duplex Annealed |
| MIL-T-81556 Revision A:1983 | Titanium and Titanium Alloys, Extruded Bars and Shapes, Aircraft Quality |
| SAE AMS6915B | Titanium Alloy Bars, Forgings and Forging Stock 7.0Al - 4.0Mo Annealed |
| SAE AMS2380G | Approval and Control of Premium-Quality Titanium Alloys |
| MIL-DTL-32528 Base Document:2015 | Rod, Bar, and Billet, Titanium Alloy TI-5111 for Use in Critical Seawater Application |
| SAE AMS6901B | Titanium Alloy Bars, Forgings, and Forging Stock 5Al - 2.5Sn, Extra Low Interstitial Annealed |
| SAE AMS6900B | Titanium Alloy Bars, Forgings and Forging Stock 5Al - 2.5Sn Annealed |
| SAE AMS6931D | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al - 4.0V Annealed |
| SAE AMS6920C | Titanium Alloy Bars, Forgings and Forging Stock 3Al - 8V - 6Cr - 4Mo - 4Zr Solution Heat Treated |
| SAE AMS6930E | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al - 4.0V Solution Heat Treated and Aged |
| SAE AMS6925B | Titanium Alloy Bars, Forgings and Forging Stock 13V - 11Cr - 3Al Solution Heat Treated |
| SAE AMS6910B | Titanium Alloy Bars, Forgings and Forging Stock 8Al - 1Mo - 1V Duplex Annealed |
| SAE AMS6907B | Titanium Alloy Bars, Forgings and Forging Stock 6.0Al - 2.0Sn - 4.0Zr - 6.0Mo Duplex Annealed |
| SAE AMS6936B | Titanium Alloy Bars, Forgings and Forging Stock 6Al - 6V - 2Sn Annealed |
| SAE AMS6906B | Titanium Alloy Bars, Forgings, and Forging Stock 6.0Al - 2.0Sn - 4.0Zr - 6.0Mo Solution Heat Treated and Aged |
| SAE AMS6921B | Titanium Alloy Bars, Forgings and Forging Stock 3Al - 8V - 6Cr - 4Mo - 4Zr Solution Heat Treated and Aged |
| SAE AMS4938A | Forgings, Titanium Alloys Heat-Treated, Finished-Part Properties: Short-Traverse Tensile, Fracture Toughness, and Longitudinal Time-Dependent-Tension |
| ASME B46.1 : 2009 | SURFACE TEXTURE (SURFACE ROUGHNESS, WAVINESS, AND LAY) |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.