SAE AMS2759/11

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Stress Relief of Steel Parts

Available format(s)

Hardcopy , PDF

Superseded date

08-11-2019

Superseded by

SAE AMS2759/11A

Language(s)

English

Published date

23-04-2014

€67.84
Excluding VAT

1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTION
8. NOTES

Sets up requirements for thermal stress relief treatments of parts manufactured from the following materials: (a) Carbon and Low Alloy Steels (b) Tool Steels (c) Precipitation Hardening, Corrosion-Resistant and Maraging Steels (d) Austenitic Corrosion-Resistant Steels, and (e) Martensitic Corrosion-Resistant Steels.

DocumentType
Standard
Pages
5
PublisherName
SAE International
Status
Superseded
SupersededBy

This specification, in conjunction with the general requirements for steel heat treatment in AMS 2759, establishes requirements for thermal stress relief treatments of parts manufactured from the following materials:aCarbon and Low Alloy SteelsbTool SteelscPrecipitation Hardening, Corrosion-Resistant and Maraging SteelsdAustenitic Corrosion-Resistant SteelseMartensitic Corrosion-Resistant Steels

MIL-DTL-32502 Base Document:2014 Coating, Cobalt-Phosphorus Alloy, Nanocrystalline (Electrodeposited)
SAE AMS2759/13 Gaseous Nitrocarburizing
SAE AMS2759/4C Heat Treatment Austenitic Corrosion-Resistant Steel Parts
NASA STD 5005(INT) : 2007 THE DESIGN AND FABRICATION OF GROUND SUPPORT EQUIPMENT
SAE AMS2759/6B Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts
SAE AMS2759E Heat Treatment of Steel Parts General Requirements
SAE AMS 2453 : 2015 LOW STRESS GRINDING OF STEEL PARTS HEAT TREATED TO 180 KSI OR OVER, AND LOW STRESS GRINDING OF CHROME PLATING APPLIED TO STEEL PARTS HEAT TREATED TO 180 KSI OR OVER
SAE AMS2759/2F Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher

ASTM A 262 : 2015 : REDLINE Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
SAE AMS2759E Heat Treatment of Steel Parts General Requirements

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.