SAE AMS2759/1E
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
HEAT TREATMENT OF CARBON AND LOW-ALLOY STEEL PARTS, MINIMUM TENSILE STRENGTH BELOW 220 KSI (1517 MPA)
22-06-2019
01-01-2009
1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Describes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa).
Committee |
AMS-E
|
DocumentType |
Standard
|
PublisherName |
SAE International
|
Status |
Superseded
|
SupersededBy |
SAE AMS6409E | STEEL, BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) SPECIAL AIRCRAFT QUALITY CLEANLINESS, NORMALIZED AND TEMPERED |
SAE AMS2759E | HEAT TREATMENT OF STEEL PARTS, GENERAL REQUIREMENTS |
SAE AMS 2453 : 2015 | LOW STRESS GRINDING OF STEEL PARTS HEAT TREATED TO 180 KSI OR OVER, AND LOW STRESS GRINDING OF CHROME PLATING APPLIED TO STEEL PARTS HEAT TREATED TO 180 KSI OR OVER |
NASA STD 5005(INT) : 2007 | THE DESIGN AND FABRICATION OF GROUND SUPPORT EQUIPMENT |
SAE AMS2759/6B | GAS NITRIDING OF LOW-ALLOY STEEL PARTS |
SAE AMS6325K | STEEL, BARS, AND FORGINGS 0.50CR - 0.55NI - 0.25MO (0.38 - 0.43C) (SAE 8740) HEAT TREATED, 105 KSI (724 MPA) TENSILE STRENGTH |
SAE MA3376C | Bolts & Screws, UNS G87400 Tensile Strength 860 MPa & 1000 MPa Procurement Specification, Metric |
SAE AMS 2424 : 2010 | PLATING, NICKEL LOW-STRESSED DEPOSIT |
SAE AMS2418J | PLATING, COPPER |
SAE AMS2759E | HEAT TREATMENT OF STEEL PARTS, GENERAL REQUIREMENTS |
SAE AMS2750E | PYROMETRY |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.