SAE AMS2759/1J
Current
The latest, up-to-date edition.
Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)
Hardcopy , PDF
English
03-08-2021
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa).
Committee |
AMS E
|
DocumentType |
Revision
|
Pages |
14
|
PublisherName |
SAE International
|
Status |
Current
|
Supersedes |