1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Specifies requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher.
Committee |
AMS-E
|
DocumentType |
Standard
|
Pages |
13
|
PublisherName |
SAE International
|
Status |
Superseded
|
SAE AMS2759E | HEAT TREATMENT OF STEEL PARTS, GENERAL REQUIREMENTS |
NASA STD 5005(INT) : 2007 | THE DESIGN AND FABRICATION OF GROUND SUPPORT EQUIPMENT |
SAE AMS2759/6B | GAS NITRIDING OF LOW-ALLOY STEEL PARTS |
SAE AMS3054C | OIL, LUBRICATING, LOW TEMPERATURE FOR -55 DEGREES C (-67 DEGREES F) SERVICE |
SAE AMS 2453 : 2015 | LOW STRESS GRINDING OF STEEL PARTS HEAT TREATED TO 180 KSI OR OVER, AND LOW STRESS GRINDING OF CHROME PLATING APPLIED TO STEEL PARTS HEAT TREATED TO 180 KSI OR OVER |
SAE AMS 2424 : 2010 | PLATING, NICKEL LOW-STRESSED DEPOSIT |
SAE AMS2418J | PLATING, COPPER |
SAE AMS2759E | HEAT TREATMENT OF STEEL PARTS, GENERAL REQUIREMENTS |
SAE AMS2750E | PYROMETRY |
SAE AMS2769B | HEAT TREATMENT OF PARTS IN A VACUUM |
SAE AMS 2759/11 : 2005 | STRESS RELIEF OF STEEL PARTS |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.