1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES

Covers the procedure and requirements for gas nitriding low-alloy and tool steels by the use of raw or dissociated ammonia.

DevelopmentNote
Supersedes SAE AMS S 6090 (06/2006) Supersedes SAE AMS 2756. (07/2008)
DocumentType
Standard
Pages
10
PublisherName
SAE International
Status
Superseded
SupersededBy
Supersedes

This document specifies the procedure and requirements for heat treating low-alloy and tool steels and for their subsequent gas nitriding by the use of raw or dissociated ammonia. Specific process parameters are given for Nitralloy 135M, Nitralloy EZ, Nitralloy N, 4140, 4340, D6AC and H11 steels. Additional alloys and steel families (e.g., stainless steels) can also be nitrided using parameters acceptable to the cognizant engineering organization.

Standards Relationship
MIL-S-6090 Revision A:1971 Similar to
MIL-H-6875 Revision H:1989 Similar to

SAE AMS2759E Heat Treatment of Steel Parts General Requirements
NASA STD 5005(INT) : 2007 THE DESIGN AND FABRICATION OF GROUND SUPPORT EQUIPMENT

ASTM E 384 : 2017 : REDLINE Standard Test Method for Microindentation Hardness of Materials
SAE AMS2418J Plating, Copper
SAE AMS2759E Heat Treatment of Steel Parts General Requirements
ASME B46.1 : 2009 SURFACE TEXTURE (SURFACE ROUGHNESS, WAVINESS, AND LAY)
SAE AMS2750E Pyrometry
SAE AMS2759/2F Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
SAE AMS2759/1E Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)
SAE ARP1820B Chord Method of Evaluating Surface Microstructural Characteristics
SAE AMS2759/9D Hydrogen Embrittlement Relief (Baking) of Steel Parts
SAE AMS2759/11 Stress Relief of Steel Parts
SAE AMS2429 BRONZE PLATE MASKING

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.