Steel, Corrosion-Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength
Available format(s)
Hardcopy , PDF
Language(s)
English
Published date
05-10-2023
Publisher
This specification covers a corrosion-resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides (thickness).
Committee |
AMS F
|
DocumentType |
Revision
|
Pages |
5
|
PublisherName |
SAE International
|
Status |
Current
|
Supersedes |
SAE AS4897B:2024 | Hose Assembly, Polytetrafluoroethylene (PTFE), Low Pressure, 450 °F and Fireproof, Procurement Specification for |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.