SAE AS 7253 : 2015
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
NUTS, SELF-LOCKING, NICKEL ALLOY, UNS N07001 CLASSIFICATION: 180 KSI/1400 DEGREES F, PROCUREMENT SPECIFICATION
Hardcopy , PDF
07-08-2020
English
01-01-2015
1. SCOPE
2. REFERENCES
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Specifies all metal, self-locking wrenching nuts, plate nuts, shank nuts, and gang channel nuts made of a corrosion and heat resistant nickel-base alloy of the type identified under the Unified Numbering System as UNS N07001.
Committee |
E-25
|
DevelopmentNote |
Supersedes SAE AMS 7253 (07/1999)
|
DocumentType |
Revision
|
Pages |
23
|
PublisherName |
SAE International
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
SAE AMS 2774 : 2016 | HEAT TREATMENT, WROUGHT NICKEL ALLOY AND COBALT ALLOY PARTS |
MIL-PRF-7808 Revision L:1997 | LUBRICATING OIL, AIRCRAFT TURBINE ENGINE, SYNTHETIC BASE |
SAE AMS 5709 : 2013 | NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS AND FORGINGS, 58NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1975 DEGREE F (1079 DEGREE C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
ASME B46.1 : 2009 | SURFACE TEXTURE (SURFACE ROUGHNESS, WAVINESS, AND LAY) |
SAE AS 3071 : 2012 | ACCEPTANCE CRITERIA - MAGNETIC PARTICLE, FLUORESCENT PENETRANT, AND CONTRAST DYE PENETRANT INSPECTION |
SAE AS 954 : 2011 | WRENCHES, HAND, TWELVE POINT, HIGH STRENGTH, THIN WALL |
NASM1312-6:2013 | FASTENER TEST METHODS, METHOD 6, HARDNESS |
ASTM E 1417/E1417M : 2016 : REDLINE | Standard Practice for Liquid Penetrant Testing |
SAE AS 8879 : 2004 | SCREW THREADS - UNJ PROFILE, INCH CONTROLLED RADIUS ROOT WITH INCREASED MINOR DIAMETER |
ASME Y14.36M : 1996 | SURFACE TEXTURE SYMBOLS |
SAE AMS 2411 : 2013 | PLATING, SILVER FOR HIGH TEMPERATURE APPLICATIONS |
SAE AS 7471 : 2015 | BOLTS AND SCREWS, NICKEL ALLOY, UNS N07001 TENSILE STRENGTH 165 KSI, CORROSION AND HEAT RESISTANT, PROCUREMENT SPECIFICATION |
SAE AMS 2410 : 2010 | PLATING, SILVER, NICKEL STRIKE, HIGH BAKE |
SAE AMS 5708 : 2015 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, WIRE FORGINGS, AND RINGS, 58NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1975 DEGREES F (1079 DEGREES C) SOLUTION HEAT TREATED |
SAE AS 1310 : 2012 | FASTENER TORQUE FOR THREADED APPLICATIONS, DEFINITIONS OF |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.