Nuts, Self-Locking, Steel, Corrosion and Heat Resistant High Strength, All Metal 1200 °F Use, UN Thread Form

Available format(s)

Hardcopy , PDF

Superseded date

13-05-2024

Superseded by

SAE AS7250E

Language(s)

English

Published date

21-11-2018

€131.37
Excluding VAT

1. SCOPE
2. REFERENCES
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES

Describes all metal, self-locking wrenching nuts, plate nuts, shank nuts, and gang channel nuts made from a corrosion and heat resistant steel of the type identified under the Unified Numbering System as UNS S66286 and of 160 ksi tensile strength at room temperature, with maximum test temperature of parts at 1200 degrees F.

DevelopmentNote
Supersedes SAE AMS 7250 (07/1999)
DocumentType
Standard
Pages
24
PublisherName
SAE International
Status
Superseded
SupersededBy
Supersedes

This document covers all metal, self-locking wrenching nuts, plate nuts, shank nuts, and gang channel nuts made from a corrosion and heat resistant steel of the type identified under the Unified Numbering System as UNS S66286 and of 160 ksi tensile strength at room temperature, with maximum test temperature of parts at 1200 °F.

SAE AMS 5737 : 2012 STEEL, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS AND TUBING, 15CR - 25.5NI - 1.2MO - 2.1TI - 0.006B - 0.30V, CONSUMABLE ELECTRODE MELTED, 1650 DEGREES F (899 DEGREES C), SOLUTION AND PRECIPITATION HEAT TREATED
SAE AS7482B Studs, Corrosion and Heat Resistant Steel, UNS S66286 Tensile Strength 130 ksi 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification
MIL-PRF-7808 Revision L:1997 LUBRICATING OIL, AIRCRAFT TURBINE ENGINE, SYNTHETIC BASE
SAE AMS5853C Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength
ASME B46.1 : 2009 SURFACE TEXTURE (SURFACE ROUGHNESS, WAVINESS, AND LAY)
SAE AS3071B Acceptance Criteria - Magnetic Particle, Fluorescent Penetrant, and Contrast Dye Penetrant Inspection
SAE AS954F Wrenches, Hand, Twelve Point, High Strength, Thin Wall
SAE AMS 5732 : 2012 STEEL, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS, TUBING AND RINGS, 15CR - 25.5NI - 1.2MO - 2.1TI - 0.006B - 0.30V, CONSUMABLE ELECTRODE MELTED 1800 DEGREES F (982 DEGREES C), SOLUTION AND PRECIPITATION HEAT TREATED
NASM1312-6:2013 FASTENER TEST METHODS, METHOD 6, HARDNESS
SAE AS7481C Studs, Steel, UNS S66286 Aged After Roll Threaded Procurement Specification For
SAE AMS 5731 : 2012 STEEL, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS, TUBING, AND RINGS, 15CR - 25.5NI - 1.2MO - 2.1TI - 0.006B - 0.30V, CONSUMABLE ELECTRODE MELTED, 1800 DEGREES F (982 DEGREES C) SOLUTION HEAT TREATED
SAE AMS2411H Plating, Silver for High Temperature Applications
SAE AS7477F Bolts and Screws, Steel, UNS S66286 Tensile Strength 130 ksi, Procurement Specification
SAE AMS2410K Plating, Silver Nickel Strike, High Bake
MIL-S-7742 Revision D:1991 SCREW THREADS, STANDARD, OPTIMUM SELECTED SERIES, GENERAL SPECIFICATION FOR
SAE AS 1310 : 2012 FASTENER TORQUE FOR THREADED APPLICATIONS, DEFINITIONS OF

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.