Creep resisting steels, nickel and cobalt alloys
Hardcopy
English
31-03-2008
This European Standard covers the grades of wrought steels and alloys listed in Table 1 and Table 2, which are usually employed for components and equipment, for which the main requirement is their creep resistance under mechanical long-time stressing at temperatures above 500 C.