Describes the ring crush test corresponding to edgewise compression strength of paperboard and intended for paperboard between 0.28 mm (0.011 in) and 0.51 mm (0.020 in) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in) and as thick as 0.76 mm (0.030 in).