UNE-EN 14179-1:2017
Current
The latest, up-to-date edition.
Glass in building - Heat soaked thermally toughened soda lime silicate safety glass - Part 1: Definition and description
Hardcopy , PDF
Spanish, Castilian, English
12-04-2017
Foreword
Introduction
1 Scope
2 Normative references
3 Terms and definitions
4 Glass products
5 Manufacturing processes
5.1 General
5.2 Toughening process
5.3 Heat soak process cycle
6 Heat soak process system
6.1 General
6.2 Oven
6.3 Glass support
6.4 Glass separation
6.5 Calibration
7 Fracture characteristics
8 Dimensions and tolerances
8.1 Nominal thickness and thickness tolerances
8.2 Width and length (sizes)
8.3 Flatness
9 Edge work, holes, notches and cut-outs
9.1 Warning
9.2 Edge working of glass for toughening
9.3 Profiled edges
9.4 Round holes
9.5 Notches and cut-outs
9.6 Shaped panes
10 Fragmentation test
10.1 General
10.2 Dimensions and number of test specimens
10.3 Test procedure
10.4 Assessment of fragmentation
10.5 Minimum values from the particle count
10.6 Selection of the longest particle
10.7 Maximum length of longest particle
11 Other physical characteristics
11.1 Optical distortion
11.2 Anisotropy (iridescence)
11.3 Thermal durability
11.4 Mechanical strength
11.5 Classification of performance under accidental
human impact
12 Marking
Annex A (normative) Heat soak process system calibration test
A.1 Calibration criteria
A.2 Loading of oven and position for glass surface temperature
measurement
A.3 Procedure
A.4 Records
A.5 Interpretation of the calibration test
Annex B (informative) Curved heat soaked thermally toughened soda
lime silicate safety glass
Annex C (informative) Examples of particle count
Bibliography
This European Standard specifies the heat soak process system together with tolerances flatness, edgework, fragmentation and physical and mechanical characteristics of monolithic flat heat soaked thermally toughened soda lime silicate safety glass for use in buildings.Information on curved heat soaked thermally toughened soda lime silicate safety glass is given in Annex B, but this product does not form part of this European Standard.Other requirements, not specified in this European Standard, can apply to heat soaked thermally toughened soda lime silicate safety glass which is incorporated into assemblies, e.g. laminated glass or insulating units, or undergo an additional treatment, e.g. coating. The additional requirements are specified in the appropriate product standard. Heat soaked thermally toughened soda lime silicate safety glass, in this case, does not lose its mechanical or thermal characteristics.Surface finished glasses (e.g. sandblasted, acid etched) after toughening are not covered by this European Standard.
| Committee |
CTN 85
|
| DocumentType |
Standard
|
| Pages |
50
|
| PublisherName |
Asociación Española de Normalización
|
| Status |
Current
|
| Standards | Relationship |
| NBN EN 14179-1 : 2005 | Identical |
| I.S. EN 14179-1:2016 | Identical |
| DIN EN 14179-1:2005-09 | Identical |
| BS EN 14179-1:2005 | Identical |
| NF EN 14179-1 : 2016 | Identical |
| EN 14179-1:2016 | Identical |
| NEN EN 14179-1 : 2016 | Identical |
| NS EN 14179-1 : 2005 | Identical |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.